Wir von der Indium Corporation glauben, dass die Materialwissenschaft die Welt verändert. In Anerkennung des bemerkenswerten Materials, das sich hinter unserem Namen verbirgt, werden wir monatliche Folgen der Elements of Indium-Serie veröffentlichen - ein Bildungsprogramm, das das Bewusstsein für die einzigartigen Anwendungen, den Reichtum und die interessanten Eigenschaften des 49sten Elements stärken soll.
Perhaps the most widely recognized compound of indium is indium-tin oxide (ITO). This ubiquitous compound is a transparent conductive oxide used in almost all flat panel displays and touchscreen devices. While ITO is the most recognized of indiums compounds, there are several others that provide solutions for a number of applications.
Indium trichloride, or IndiTri, is a versatile compound needed by a number of industries in a wide range of applications, including LEDs, lighting, and semiconductor component manufacturing. IndiTri is commonly used as a starting compound for the synthesis of other inorganic and organic indium compounds, such as tri-methyl indium (TMI), the most widely used metal-organic precursor for indium. IndiTri is also used as an additive to alkaline batteries to reduce outgassing and improve operational efficiency of the battery when under electrical load.
The first step to the well-known ITO, indium oxide, or IndiOx, is a compound that can be doped with tin oxide to form ITO sputtering targets for thin-film coating. On its own, IndiOx can be used to suppress gas formation in alkaline batteries, as a color additive for glass, and as an anti-arcing additive in high-current electrical switches and contacts.
For electroplating applications, indium sulfate, or IndiSul, is commonly used as a compound in chemical synthesis and proprietary plating chemistries to enable electroplating of indium layers onto a variety of substrates. It can also be used as a hardening agent in gold plating baths.
Indium Corporation is a global leader for indium metal and associated technologies. For more information on indium metal, visit indiumstg.wpenginepowered.com/indium49.
Über Indium Corporation
Die Indium Corporation ist ein führender Materialveredler, -schmelzer, -hersteller und -lieferant für die weltweiten Elektronik-, Halbleiter-, Dünnschicht- und Wärmemanagementmärkte. Zu den Produkten gehören Lote und Flussmittel, Hartlote, Materialien für thermische Schnittstellen, Sputtertargets, Metalle und anorganische Verbindungen aus Indium, Gallium, Germanium und Zinn sowie NanoFoil. Das 1934 gegründete Unternehmen verfügt über einen weltweiten technischen Support und Fabriken in China, Deutschland, Indien, Malaysia, Singapur, Südkorea, dem Vereinigten Königreich und den Vereinigten Staaten.
Weitere Informationen über die Indium Corporation finden Sie unterindiumstg.wpenginepowered.comoder per E-Mail beiJingya Huang. Sie können auch unseren Experten von „From One Engineer To Another“ (, #FOETA) unterwww.linkedin.com/company/indium-corporation/oder@IndiumCorp folgen.