Indium6.4 Water-Soluble Solder Paste’s flux chemistry minimizes voiding under QFN and BGA assemblies. A typical water-soluble solder paste has approximately 15-30 percent voiding; however, Indium6.4 consistently yields less than five percent.
Indium6.4 provides:
- Fewer voids
- Smaller voids
- Good cleanability and reflow properties
- Exceptional response-to-pause printing
- Extended stencil life
- Exceptional slump resistance
Indium6.4 is manufactured with standard type 3 powder in Sn63, Sn62, and Indalloy100 (tin, lead, and silver). It joins Indium6.3 as one of Indium Corporation’s top-performing water-soluble solder pastes.
For more information on Indium6.4 and our other Indium Corporation solder pastes, visit indiumstg.wpenginepowered.com/Indium6.4.
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, solar, thin-film, and thermal management markets. Products include solders, preforms, and fluxes; brazes; sputtering targets; indium, gallium, and germanium metals and inorganic compounds; and NanoFoil®. Founded in 1934, Indium has global technical support and factories located in China, Singapore, South Korea, the United Kingdom, and the USA.
Para obtener más información sobre Indium Corporation, visita indiumstg.wpenginepowered.com o envía un correo electrónico a [email protected].