Les gens,
Many peopleresponded to my recent post, In Search of Tin Whisker Fails in Lead-Free Soldering. A few pointed out thatthe recent NASA report on the Toyota Unintended Acceleration Issuediscussed numerous tin whiskers that were found, one implicated in a failure. The tin whiskers wereemanating fromtin plating.
We don't know, however, if tin whisker mitigation techniques wereused. In a mission critical application, such as this, it would appear unwise to use RoHS-compliant electronics, especially since they are not required for automobiles. In other words, autos are exempt from RoHS. Let me be very clear, from a tin whisker perspective,I am uncomfortable with RoHS-compliant tin plating in mission critical applications. Much more work needs to be done before such tin plating should be used in mission critical applications.
In addition, in response to my post, a number of peoplepointed out the difficulty of proving a tin whisker fail and the reluctance of any manufacturer to admit that their products had them.
But my quest remains unfulfilled; the question remains:
"… who knows of any verified tin whisker fails when tin whisker mitigation techniques where used?Tin whisker mitigation techniques typically use 2% bismuth or antimony in the tin, assure that the tin has a matte finish and use a nickel strike plating between the copper and the tin to minimize copper diffusion into the tin."
Restated, here is my point. Since RoHS, quite a few people take a position something like this:
With RoHS-compliant assembly, even the world of non-mission critical electronics is at considerable risk of numerous catastrophic failures, due to tin whiskers, that will cost $100s billions.
Istill maintain, that with mitigation techniques, such as recommended by iNEMI, tin whisker control, for non-critical electronics, can be manageable.
AsIpack up to leave my office today at Thayer Engineering School at Dartmouth, Iam across the aisle from the chaps that provide our computers and ITsupport. They buy millions of dollars of electronics a year. In chatting with them they state two things:
1. They have noted no difference in electronics reliability since RoHS implementation
2. On the very rare occasion that they get an electronics failure, it is almost always a hard drive.
Bottom line: Except for hard drives, modern electronics are very reliable for their use life.
Iexpect my quest will uncover some tin whisker fails, even with mitigation, but the fails will most likely be isolated and not a significant threat to the industry at large.
Santé,
Dr. Ron
The image is from Dr. Henning Leidecker of NASA, one of the world's leading tin whisker experts.