As an advanced materials innovator and a premier global supplier to the mobile device assembly market, Indium Corporation is proud to be included in the Smithsonian National Museum of Natural History’s Cellphone: Unseen Connections special exhibit in Washington D.C., on display through 2026.
Specifically, Indium Corporation’s Indium Tin Oxide (ITO) is highlighted by the museum. The touchscreens ubiquitous on modern smart phones include many layers, including a transparent, conductive ITO film arranged in an invisible grid on top of the display. When a user touches the surface, that contact alters the capacitance, or stored energy, of an electronic circuit which determines the position of the user’s finger. In addition to ITO powder, Indium Corporation provides numerous cutting-edge materials for mobile device assembly, including an award-winning, low-temperature solder alloy system.
Not only is the company’s ITO powder on display, Indium Corporation team members are also integrated into the exhibit. Robert Ploessl, Product Manager for Metals and Compounds, is prominently featured as both a subject matter expert and representative of Indium Corporation.
“The Smithsonian is a prestigious institution and, as a self-proclaimed science geek, it is a tremendous honor to be included in this fascinating exhibit,” said Ploessl. “When you touch your screen to connect with others, you touch our materials. I am very proud of that.”
Through authentic artifacts, immersive and digital experiences, and data visualization, Cellphone: Unseen Connections illuminates the world of cell phones at the intersection of science, art, technology, and society. The exhibit consists of more than 750 objects from around the world, multimedia installations, an interactive group chat, and a graphic novel spanning three gallery walls. The Smithsonian National Museum of Natural History offers free admission and is open every day except for Christmas.
關於 Indium Corporation
Indium Corporation 是全球電子、半導體、薄膜和熱管理市場的主要材料精煉商、冶煉商、製造商和供應商。產品包括焊料和助熔劑;銅钎;熱介面材料;濺鍍靶材;铟、鎵、锗、錫金屬和無機化合物;以及 NanoFoil 。公司成立於 1934 年,擁有全球性的技術支援,工廠分佈於中國、德國、印度、馬來西亞、新加坡、南韓、英國和美國。
如需更多關於 Indium Corporation 的資訊,請造訪www.indium.com或寄電子郵件給Jingya Huang。您也可以透過www.linkedin.com/company/indium-corporation/或@IndiumCorp 追蹤我們的專家,From One Engineer To Another (#FOETA)。