Indium Corporation has added to its line of thermal interface materials (TIMs) with the introduction of HSMF-OS, a non-silicone based metal/polymer material designed for burn-in and test applications.
HSMF-OS is designed for high insertion capability. Its high tensile strength and soft compliant polymer backing allow it to survive multiple insertions. HSMF-OS has been tested to withstand over 5,000 insertion cycles without any loss of performance.
One of the challenges associated with a burn-in TIM is the attachment method. HSMF-OS has inherent adhesive properties on one side that allow for hand placement, removing the need for these additional steps and fixtures without compromising thermal performance. The opposite side is aluminum and it will not mark or stain the DUI (device under test).
HSMF-OS offers consistently good performance without phase change.
For more information on HSMF-OS and Indium Corporation’s full line of TIMs, visit indiumstg.wpenginepowered.com/TIMs.
Die Indium Corporation ist ein führender Materialhersteller und -lieferant für die weltweiten Märkte für Elektronik, Halbleiter, Dünnschichten und Wärmemanagement. Zu den Produkten gehören Lote und Flussmittel, Hartlote, Materialien für thermische Schnittstellen, Sputtertargets, Metalle und anorganische Verbindungen aus Indium, Gallium, Germanium und Zinn sowie NanoFoil®. Das 1934 gegründete Unternehmen verfügt über einen weltweiten technischen Support und Fabriken in China, Malaysia, Singapur, Südkorea, dem Vereinigten Königreich und den USA.
Weitere Informationen über die Indium Corporation finden Sie unterindiumstg.wpenginepowered.comoder per E-Mailan [email protected]. Sie können unseren Experten von „From One Engineer ToAnother®“(#FOETA) auch unterwww.facebook.com/indiumoder@IndiumCorp folgen.