Indium Corporation Features InFORMS Reinforced Solder Preforms at APEC 2017

Indium Corporation will feature its reinforced solder alloy fabrications, InFORMS®, at APEC 2017, March 26-30, in Tampa, Fla.

InFORMS are reinforced solder preforms that increase lateral strength and stability. As a result, improved thermal cycling reliability can be achieved.

In one study where InFORMS were used to solder a DBC to the baseplate of an IGBT, the following were achieved:

  • Fiabilidad del ciclo térmico 4 veces mejorada en comparación con un enfoque basado únicamente en preformas de soldadura.
  • Fiabilidad del ciclo térmico 2x mejorada en comparación con un enfoque de preforma de soldadura + puntada de unión de alambre de Al.
  • Low-voiding of <1%
  • Lower cost of ownership – an InFORM is a drop-in replacement for a standard preform or solder paste, requiring no additional process steps or equipment

For more information about InFORMS, visit indiumstg.wpenginepowered.com/informs or visit Indium Corporation at booth #525.

Para obtener más información sobre Indium Corporation, visitaindiumstg.wpenginepowered.como envía un correo electrónicoa [email protected]. También puedes seguir a nuestros expertos, From One Engineer ToAnother®(#FOETA), enwww.facebook.com/indiumo en@IndiumCorp.