Indium Corporation’s Mary Ma Awarded Best Paper at SMTA China East Technology Conference 2018

Indium Corporation’s Mary Ma, Research Chemist, was presented with the “Best Paper” award at the SMTA China East Technology Conference 2018 on April 23-26 in Shanghai, China.

Ma’s paper, Sn3.2Ag0.7Cu5.5Sb Solder Alloy with High Reliability Performance up to 175°C, reviewed the testing results of her efforts to achieve high-reliability under a wide range of high-temperatures using the lead-free solder alloy also known as Indalloy®276. Her paper found that in order to achieve this, it is imperative to balance a solder alloy’s ability to handle tensile stress versus its rigidity.

Ma joined Indium Corporation in 2010 and is based in Suzhou, China. She is responsible for developing halogen-free, lead-free, and no-clean flux chemistries with low-voiding. Ma earned her bachelor’s degree in Chemistry from Qufu Normal University and her master’s degree in Physical Chemistry from Nanjing University.

Indium Corporation es uno de los principales fabricantes y proveedores de materiales para los mercados mundiales de la electrónica, los semiconductores, las películas finas y la gestión térmica. Sus productos incluyen soldaduras y fundentes, soldaduras fuertes, materiales de interfaz térmica, cátodos para sputtering, metales y compuestos inorgánicos de indio, galio, germanio y estaño, y NanoFoil®. Fundada en 1934, la empresa cuenta con asistencia técnica mundial y fábricas en China, Malasia, Singapur, Corea del Sur, Reino Unido y Estados Unidos.

Para obtener más información sobre Indium Corporation, visitaindiumstg.wpenginepowered.como envía un correo electrónicoa [email protected]. También puedes seguir a nuestros expertos, From One Engineer ToAnother®(#FOETA), enwww.facebook.com/indiumo en@IndiumCorp.