コンテンツへスキップ

Indium Corporation’s Mary Ma Awarded Best Paper at SMTA China East Technology Conference 2018

Indium Corporation’s Mary Ma, Research Chemist, was presented with the “Best Paper” award at the SMTA China East Technology Conference 2018 on April 23-26 in Shanghai, China.

Ma’s paper, Sn3.2Ag0.7Cu5.5Sb Solder Alloy with High Reliability Performance up to 175°C, reviewed the testing results of her efforts to achieve high-reliability under a wide range of high-temperatures using the lead-free solder alloy also known as Indalloy®276. Her paper found that in order to achieve this, it is imperative to balance a solder alloy’s ability to handle tensile stress versus its rigidity.

Ma joined Indium Corporation in 2010 and is based in Suzhou, China. She is responsible for developing halogen-free, lead-free, and no-clean flux chemistries with low-voiding. Ma earned her bachelor’s degree in Chemistry from Qufu Normal University and her master’s degree in Physical Chemistry from Nanjing University.

インジウム・コーポレーションは、世界のエレクトロニクス、半導体、薄膜、熱管理市場に材料を供給する一流メーカーです。製品には、はんだおよびフラックス、ろう材、熱界面材料、スパッタリングターゲット、インジウム、ガリウム、ゲルマニウム、スズの金属および無機化合物、NanoFoil®などがある。1934年に設立され、グローバルな技術サポートと中国、マレーシア、シンガポール、韓国、英国、米国に工場を持つ。

インジウム・コーポレーションに関する詳細については、indiumstg.wpenginepowered.comをご覧いただくか、[email protected] までメールでお問い合わせください。また、当社の専門家による「From One Engineer ToAnother®(#FOETA)」を、www.facebook.com/indiumまたは@IndiumCorp でフォローすることもできます。