Indium Corporation is a small- to mid-volume supplier of specialty solder spheres. We offer a very wide variety of alloys and size range capabilities from around 0.004″ (100 μm) to 0.063″ (1.6 mm), depending on the alloy. Melting points range from below 90°C to over 700°C.
Powered by Indium Corporation
- Sphère à faible teneur en oxyde
- Contrôle étroit de la tolérance du diamètre
- Contrôle rigoureux de la composition des alliages

Vue d'ensemble
Caractéristiques et avantages
Specialty solder spheres are used in a variety of market segments, including medical, transportation and automotive, military and aerospace, high-end mobile, and computing. Clean manufacturing and processing ensure low-oxide levels with no organic contamination. All spheres are manufactured in IATF-16949 certified facilities.
- Diamètres précis
- Capable of supplying quantities from 1 sphere to > 20 million per month
- La propreté de la fabrication et du traitement garantit des niveaux d'oxyde faibles et l'absence de contamination organique.
- La finition et l'emballage en salle blanche garantissent la continuité de la propreté
- Les métaux purs garantissent des sphères finies de haute qualité
- Fabriqué dans des installations certifiées IATF-16949
Produits de la sphère de soudure
Alliages sans plomb
| Alliage | Indalloy® # | Melting Point Solidus (°C) | Melting Point Liquidus (°C) | Min (in)* | Max (in)* | Min (µm)* | Max (µm)* |
|---|---|---|---|---|---|---|---|
| In50Sn | 1 | 118 | 125 | 0.004 | 0.030 | 102 | 762 |
| In48Sn (In/Sn eutectic) | 1E | 118 | 0.004 | 0.035 | 102 | 889 | |
| Bi42Sn (Bi/Sn eutectic) | 281 | 138 | 0.008 | 0.109 | 203 | 2,769 | |
| Bi42Sn1Ag | 282 | 139 | 140 | 0.008 | 0.030 | 203 | 762 |
| 99.99In (“Pure Indium”) | 4 | 157 | 0.004 | 0.050 | 102 | 1,270 | |
| Sn20In2.8Ag (Pb-free “Sn63”) | 227 | 175 | 187 | 0.004 | 0.030 | 102 | 762 |
| Sn3.0Ag0.5Cu (SAC305) | 256 | 217 | 220 | 0.004 | 0.065 | 102 | 1,651 |
| Sn4.0Ag0.5Cu (SAC405) | 2562 | 217 | 225 | 0.004 | 0.035 | 102 | 889 |
| Sn4Ag | 121 | 221 | 228 | 0.004 | 0.021 | 102 | 533 |
| Sn5Ag | 132 | 221 | 240 | 0.004 | 0.032 | 102 | 800 |
| 80Au20Sn (Au/Sn eutectic) | 182 | 280 | 0.004 | 0.039 | 102 | 991 |
*Gamme approximative de diamètres manufacturables
Alliages contenant du plomb
| Alliage | Indalloy® # | Melting Point Solidus (°C) | Melting Point Liquidus (°C) | Min (in)* | Max (in)* | Min (µm)* | Max (µm)* |
|---|---|---|---|---|---|---|---|
| Sn46Pb8Bi | 240 | 160 | 173 | 0.010 | 0.030 | 254 | 762 |
| Sn36Pb2Ag (Sn62) | Sn62 | 179 | 181 | 0.004 | 0.030 | 102 | 762 |
| Sn37Pb (63Sn) | 106 | 183 | 0.004 | 0.050 | 102 | 1,270 | |
| Pb25In | 110 | 183 | 192 | 0.004 | 0.027 | 102 | 686 |
| Pb40In | 206 | 197 | 231 | 0.004 | 0.020 | 102 | 508 |
| Pb10Sn | 159 | 275 | 302 | 0.004 | 0.040 | 102 | 1,016 |
*Gamme approximative de diamètres manufacturables
Fiches techniques des produits
Specialty Solder Spheres PDS 97549 R10
Applications connexes
Marchés connexes
Le soutien d'experts pour des résultats fiables
Vous avez des questions techniques ou commerciales ? Notre équipe dévouée est là pour vous aider. "D'un ingénieur à l'autre®" n'est pas seulement notre devise, c'est notre engagement à fournir un service exceptionnel. Nous sommes prêts quand vous l'êtes. Connectez-vous !

Vous cherchez des fiches de données de sécurité ?
Accédez à tout ce dont vous avez besoin - des spécifications techniques aux conseils d'application - en un seul endroit pratique.

Votre réussite
est notre objectif
Optimisez vos processus grâce aux matériaux et aux technologies les plus récents, ainsi qu'à l'assistance d'experts en matière d'applications. Tout commence par un contact avec notre équipe.