Indium Corporation has earned a Mexico Technology Award for its fast wetting, no-clean cored wire with spatter control technology, CW-818. The award was presented on Wednesday, Sept. 21 at the SMTA Guadalajara Expo and Tech Forum hosted at the Hilton Guadalajara in Jalisco, Mexico.
“At Indium Corporation, we believe that materials science can change the world,” said Robert McKerrow, Senior Product Specialist Flux-Cored Wire, Wave Solder Flux, and Bar Solder. “We are honored to receive the Mexico Technology Award for CW-818 as it provides further proof that our products are continuing to make an indelible mark on the industry.”
メキシコ・テクノロジー・アワードは、メキシコEMSが主催するもので、プリント回路アセンブリおよびパッケージング業界における過去1年間の最も優れた新機軸を表彰するものである。
Indium Corporation’s CW-818 is designed to meet the demanding requirements of today’s manual and robotic soldering processes. CW-818 provides fast wetting speeds, allowing users to minimize cycle times. The spatter control technology minimizes flux spattering while the heat-resistant nature of the formula reduces flux build-up on the soldering iron tip, and also leaves a clear, non-tacky residue post-soldering (even when using a high iron tip temperature). The combination of superior soldering performance, improved overall cleanliness, and excellent visual appearance post-soldering delivers a truly no-clean flux-cored wire.
インジウムコーポレーションの広範な製造工程管理により、CW-818コアードワイヤーは、工程設定上の課題を最小限に抑え、歩留まりを最大化しながら、正確なはんだ量を提供します。CW-818はボイドがなく、直径と層巻きが一定しているため、ロボットはんだ付け装置に引き込まれた際のフラックス不足やよじれによる停止を防ぎます。その結果、極めて信頼性の高い強固なはんだ接合が実現します。
インジウム・コーポレーションについて
インジウム・コーポレーションは、世界のエレクトロニクス、半導体、薄膜、熱管理市場向けの一流の材料精製、製錬、製造、サプライヤーである。製品には、はんだおよびフラックス、ろう材、熱界面材料、スパッタリングターゲット、インジウム、ガリウム、ゲルマニウム、スズの金属および無機化合物、NanoFoil などがある。1934年に設立され、グローバルな技術サポートと中国、ドイツ、インド、マレーシア、シンガポール、韓国、英国、米国に工場を持つ。
インジウム・コーポレーションについての詳細は、www.indium.comをご覧いただくか、Jingya HuangまでEメールにてお問い合わせください。また、当社の専門家であるFrom One Engineer To Another (#FOETA)を、www.linkedin.com/company/indium-corporation/または@IndiumCorp でフォローすることもできます。