Indium Corporation will feature its new Flip-Chip Flux WS-446HF and Ball Attach Flux WS-823 at Productronica China, March 20-22, in Shanghai, China.
Indium Corporation’s WS-446HF is a water-soluble, halogen-free, flip-chip dipping flux with an activator system powerful enough to promote good wetting on the most demanding surfaces – including solder-on-pad (SoP), Cu-OSP, ENIG, embedded trace substrates (ETS), and flip-chip on leadframe applications. WS-446HF provides:
- Excellent solderability to reduce open joints
- Tackiness suitable for holding large die in place during assembly and reducing die tilt
- Chemistry that eliminates dendrite issues
- Reduced voiding
- Good cleanability
WS-823 is a water-soluble, halogen-free, ball-attach flux designed for use in pin transfer and printing applications for ball attachment to both substrates (BGA manufacturing) and wafers for WLP (wafer-level packaging). WS-823 offers:
- Excellent solderability on some of the most demanding substrate metallizations, such as copper OSP
- Lower process costs and warpage due to the elimination of “pre-fluxing”
- Consistent flux deposition
- Good tack during heating combined with fast soldering eliminates missing ball
- Low-cost simplified cleaning
Both WS-446HF and WS-823 are cleanable with just DI water only.
For more information on Indium Corporation’s fluxes, visit indiumstg.wpenginepowered.com/flux-and-epoxy/ or visit Indium Corporation’s booth #E2.2514.
Die Indium Corporation ist ein führender Materialhersteller und -lieferant für die weltweiten Märkte für Elektronik, Halbleiter, Dünnschichten und Wärmemanagement. Zu den Produkten gehören Lote und Flussmittel, Hartlote, Materialien für thermische Schnittstellen, Sputtertargets, Metalle und anorganische Verbindungen aus Indium, Gallium, Germanium und Zinn sowie NanoFoil®. Das 1934 gegründete Unternehmen verfügt über einen weltweiten technischen Support und Fabriken in China, Malaysia, Singapur, Südkorea, dem Vereinigten Königreich und den USA.
Weitere Informationen über die Indium Corporation finden Sie unterindiumstg.wpenginepowered.comoder per E-Mailan [email protected]. Sie können unseren Experten von „From One Engineer ToAnother®“(#FOETA) auch unterwww.facebook.com/indiumoder@IndiumCorp folgen.