When it comes to shots at Indium Corporation, it is not about bullets, vaccines, or vodka; it’s about small spherical or tear-drop shaped forms of metals and alloys. While ingots and cakes are more popular forms when we think about metals and alloys, shots have their exclusive benefits.
Shots provide a larger area-to-volume ratio for the metals and alloys that favor the interaction with external factors. Afterall, dissolving a certain volume of metal in a solution is much easier and faster with small pieces than with a single bulk quantity. For instance, considering a 500g indium ingot with dimensions of 7” × 1.25” × 0.5” versus several indium shots of 0.125” diameter with the same total weight, the ratio of surface area exposed to the solution is nearly 8 times higher for shots. Therefore, if surface area is the limiting factor in dissolving indium in a chemical solution, shots would ideally dissolve 8 times faster.
작은 용융 포트를 사용하는 엔지니어는 잉곳이 너무 커서 맞지 않을 때 샷을 사용하면 도움이 됩니다. 샷은 공급량에서 더 나은 해상도를 제공합니다. 더 큰 형태의 금속 및 합금에서는 달성하기 어려운 소량으로 샷의 무게를 보다 정확하게 측정할 수 있습니다. 또한 잉곳 파일링 후 발생하는 스크랩을 줄이는 데 도움이 됩니다. 그 외에도 구형 또는 물방울 모양의 금속 및 합금을 사용하면 보관, 취급 및 공급이 훨씬 더 편리합니다.
샷은 일반적으로 작은 원형 구멍을 통해 용융된 형태의 금속을 강제로 주입하여 생산합니다. 그런 다음 용융물은 냉각 용액을 통과하여 샷으로 응고됩니다. 샷은 안정성과 경화를 위해 건조, 어닐링 또는 추가 가공을 거칩니다. 원형 구멍의 크기와 용액을 따라 통과하는 길이에 따라 샷의 크기와 모양이 결정됩니다.
Shots in general have a lower shelf-life compared to larger-sized forms because of the larger exposed area, which increases the interaction with external elements like oxygen, humidity, etc.
Indium Corporation produces spherical and tear-drop shaped shots for different metals and alloys. This list includes, but is not limited to, indium, gallium, germanium, tin, Indalloy®117, Indalloy®136, and Indalloy®158. The purity that we provide ranges from 3N to 6N5. Readily available shots are approximately 0.125” in diameter and can be adjusted based on customer requirements and quantity. We can also manage the uniformity in size as required.