Indium Corporation, a leading materials provider for the electronics assembly market, recently earned two CIRCUITS ASSEMBLY New Product Introduction (NPI) Awards for its high-reliability alloy used for solder paste, Durafuse® HR, and its high-reliability, halide and halogen-free flux-cored wire, CW-807RS.
The NPI Awards recognize the leading new products for electronics assembly during the past 12 months. An independent panel of practicing engineers selects honorees based on a variety of criteria, including creativity and innovation, design, and performance. With an extended history of NPI Awards highlighting its commitment to innovation, Indium Corporation is proud to receive two more honors in 2025, further strengthening its position as a leader in electronics assembly materials.
“Our belief that materials science can change the world is exemplified by every one of our products,” said Indium Corporation President and CEO Ross Berntson. “CW-807RS delivers unmatched soldering speed, spatter control, and overall cleanliness, while Durafuse® HR is a breakthrough alloy that improves thermal cycling performance and reduces voiding, providing game-changing solutions for high-reliability applications. We’re excited to offer these innovations to make a lasting impact on our customers and the industry.”
Durafuse® HR is a high-reliability solder alloy developed from the company’s Durafuse® mixed-alloy technology. Engineered to deliver enhanced thermal cycling performance and superior voiding performance without vacuum reflow, Durafuse® HR is designed specifically for the rigorous demands of automotive electronics and other high-reliability applications. It is ideal for manufacturers transitioning from SAC305, requiring only minimal process adjustments for easy implementation.
Among its key features, Durafuse® HR offers:
- Exceptional thermal cycling reliability, withstanding 3,000+ cycles at -40°C–125°C
- Reduced bottom-terminated component (BTC) voiding, even without vacuum reflow
- Superior shear strength for increased durability and reduced solder joint cracking
- Compatibility with most SAC305 reflow profiles and common PCB surface finishes (ImSn, OSP, ENIG) while allowing for fine-tuning to meet precise process requirements.
- Optimized yield rates and reliability, reducing defects, rework, and overall production costs
CW-807RS is a next-generation high-reliability, halide, and halogen-free flux-cored wire designed to improve wetting speeds and cycle times in electronics assembly and robotic soldering applications. Built upon the proven performance of the CW-807 and CW-818 formulas, CW-807RS features fast wetting and enhanced spatter control technology for a cleaner, more efficient soldering process.
Among its key features, CW-807RS offers:
- Faster wetting speeds for improved cycle times
- Minimal spattering and clear to light-colored residue for an aesthetically clean finish
- Excellent solderability in manual and robotic applications requiring an “L0” IPC classification
- Versatility across a wide range of alloys and diameters to meet diverse assembly needs
- Industry-leading reliability, passing stringent test requirements with no dendritic growth or visible corrosion
Discover how Indium Corporation’s award-winning Durafuse® HR and CW-807RS are setting new standards in high-reliability electronics assembly: visit indiumstg.wpenginepowered.com to learn more about these innovative solutions.
인듐 코퍼레이션 소개
Indium Corporation® is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, Germany, India, Malaysia, Singapore, South Korea, the United Kingdom, and the U.S.
인듐 코퍼레이션(Indium Corporation)에 대한 자세한 정보는 indiumstg.wpenginepowered.com을 방문하거나 [email protected]으로 이메일을 보내 주시기 바랍니다. 또한 www.linkedin.com/company/indium-corporation/에서 당사의 전문가 그룹인 ‘From One Engineer ToAnother® (#FOETA)’를 팔로우하실 수 있습니다.