콘텐츠로 건너뛰기

인듐 코퍼레이션 전문가들, ‘프로덕트로니카 2017’에서 발표 예정

Indium Corporation’s Andreas Karch, Regional Technical Manager, Germany, Austria and Switzerland, and Karthik Vijay, Technical Manager, Europe, Africa and the Middle East, will present at Productronica, November 14-17, in Munich, Germany.

Indium Corporation’s Karch and Vijay will present the following:

  • A Novel Solder Alloy for Service Temperatures of 150–175°C in Automotive Applications
    • German presentation by Karch
      Wednesday, November 15 at 5 p.m.
    • English presentation by Vijay
      Thursday, November 16 at 5 p.m.
  • Minimizing QFN Voiding During SMT Assembly
    • German presentation by Karch
      Tuesday, November 14 at 4 p.m.
    • English presentation by Vijay
      Wednesday, November 15 at 4 p.m.

Karch provides technical support for customers in Germany, Austria and Switzerland, sharing process knowledge and making technical recommendations for the use of Indium Corporation’s materials, such as solder paste, solder preforms, fluxes, and thermal management materials. Karch has more than 20 years of automotive industry experience, including the advanced development of customized electronics. He is an ECQA-certified integrated design engineer and has a Six Sigma Yellow Belt. The Austrian Patent Office also selected him as one of the 2014 recipients of the Top 10 Inventum Awards for an automotive LED assembly. Karch maintains a thorough understanding of process technologies and project management skills.

Vijay is based in the UK and manages Indium Corporation’s technology programs and technical support throughout Europe. His expertise is focused on solder paste, engineered solders, thermal interface materials, and semiconductor-grade electronics assembly materials. Karthik is active in several industry organizations, including IMAPS and the Surface Mount Technology Association (SMTA), and has presented at industry forums and conferences internationally. He earned his master’s degree in systems science and industrial engineering from Binghamton University, State University of New York.

Indium Corporation은 전 세계 전자, 반도체, 박막 및 열 관리 시장에 최고의 소재를 제조 및 공급하는 기업입니다. 주요 제품으로는 솔더 및 플럭스, 브레이즈, 열 인터페이스 재료, 스퍼터링 타겟, 인듐, 갈륨, 게르마늄, 주석 금속 및 무기 화합물, NanoFoil® 등이 있습니다. 1934년에 설립된 Indium은 중국, 말레이시아, 싱가포르, 한국, 영국, 미국에 글로벌 기술 지원 및 공장을 보유하고 있습니다.

인듐 코퍼레이션(Indium Corporation)에 대한 자세한 정보는indiumstg.wpenginepowered.com을방문하거나[email protected]으로 이메일을 보내 주시기 바랍니다. 또한www.facebook.com/indium또는@IndiumCorp에서 당사의 전문가 그룹인 From One Engineer ToAnother®(#FOETA)를 팔로우하실 수 있습니다.