Indium Corporation will feature its new solder paste, Indium10.1, at the Surface Mount Technology Association’s International Conference and Exhibition (SMTAi) from Sept. 28-Oct. 2 in Rosemont, IL.
Indium10.1 is a Pb-free halogen-containing solder paste with the lowest levels of voiding for QFNs, BGAs, and pads with large ground planes.
The oxidation-inhibiting properties of Indium10.1 provide industry-leading head-in-pillow and graping resistance, with complete coalescence, even after long reflow profiles. Indium10.1’s exceptional soldering ability makes it the best solution for components with less-than-ideal solderability and challenging RF shield metallizations.
Indium10.1 offers the lowest cost of ownership to PCB assembly manufacturers through best-in-class printing and soldering performance, including industry-leading print definition and transfer efficiency, low voiding performance, and head-in-pillow and graping resistance.
Indium Corporation will be exhibiting at booth 430.
For more information about Indium10.1 or the Pb-free Solder Paste series, visit indiumstg.wpenginepowered.com/solder-paste-and-powders/leading-pb-free-solder-pastes/ or email [email protected].
인듐 코퍼레이션(Indium Corporation)에 대한 자세한 정보는 indiumstg.wpenginepowered.com을 방문하거나 [email protected]으로 이메일을 보내 주시기 바랍니다.