Indium Corporation Technology Expert to Host Webinar on Flux Reliability

Indium Corporation Senior Technical Support Engineer Eric Bastow will present his IPC APEX EXPO 2010 and 2011 technical papers as part of IPC’s Summer School webinar series on Wednesday, August 10, 2011, from 10 to 11 a.m. CST (11 a.m. to noon EST).

Eric will present Effects of Flux Residues on Reliability, which discusses the implications of an experiment designed to study the effects of entrapping a no-clean flux residue under a component body or RF shield, as it relates to the surface insulation resistance (SIR) performance of the flux residue.

His second paper, Understanding SIR, discusses the issue of SIR coupon preparation, board cleaning techniques, and how board cleanliness directly affects SIR results. The differences between two of the industry’s most common SIR specifications, the subjective nature of SIR testing on water washable/soluble materials and testing for SIR when the assembly process has multiple residue sources will also be covered.

As a Senior Technical Support Engineer, Eric provides support for Indium’s full range of solder products for the electronics assembly, semiconductor packaging, and thermal management markets.

Eric is an SMTA-certified process engineer (CSMTPE) and is certified as a Six Sigma Green Belt from Dartmouth College’s Thayer School of Engineering. He is also a certified IPC-A-600 and 610D Specialist. Eric has an associate’s degree in Engineering Science from the State University of New York and has authored several technical papers and articles.

Eric has experience in developing new solder paste flux chemistries, performing residual gas analysis of hermetic electronic packages and developing electroless nickel-plating bath chemistries. Eric is based at Indium Corporation’s global headquarters in Clinton, NY. He also authors a technology blog, which can be found at blogs.indium.com/blog/eric-bastow.

The registration fee for the webinar is $75 per login for IPC members and $100 per login for non-members. For more information or to register, visit www.ipc.org.

Indium Corporation은 전 세계 전자, 반도체, 태양광, 박막 및 열 관리 시장에 최고의 소재를 공급하는 기업입니다. 주요 제품으로는 솔더, 프리폼 및 플럭스, 브레이즈, 스퍼터 타겟, 인듐, 갈륨, 게르마늄 화학물질 및 소싱, 반응성 나노포일® 등이 있습니다. 1934년에 설립된 Indium은 중국, 싱가포르, 한국, 영국, 미국에 글로벌 기술 지원 및 공장을 보유하고 있습니다.

인듐 코퍼레이션(Indium Corporation)에 대한 자세한 정보는 indiumstg.wpenginepowered.com을 방문하거나 [email protected]으로 이메일을 보내 주시기 바랍니다.