Indium Corporation will feature its ultra-reliable Indium8.9HF Solder Paste at NEPCON South China, August 28-30, in Shenzhen, China.
Indium8.9HF Solder Paste is an air reflow, no-clean solder paste specifically formulated to accommodate the higher processing temperatures required by the SnAgCu, SnAg, and other alloy systems favored by the automotive electronics industry.
The Indium8.9HF series delivers no-clean, halogen-free solder paste solutions designed to produce low-voiding—plus improved stability—during the printing process. Indium8.9HF:
- Demonstrates consistent printing and reflow performance for up to 12 months in refrigerated storage
- 실온에서 한 달 동안 보관해도 우수한 인쇄 및 리플로우 성능 유지
- 스텐실에 60시간 동안 방치한 후에도 뛰어난 응답성-일시 정지 인쇄 성능 제공
With all these qualities, Indium8.9HF solder paste is able to enhance the reliability of automotive products in three ways:
- Improved thermal conductivity and thermal reliability with industry-proven low-voiding performance
- Enhanced mechanical reliability when paired with Indium Corporation’s newest high-reliability alloy, Indalloy®276, which allows for a stable and consistent performance under a harsh environment (Indalloy®276 is ideal for operating temperatures equal to or greater than 125°C)
- Higher electrical reliability with an enhanced SIR
Additionally, Indium Corporation will spotlight Indium10.1HF Solder Paste—an air reflow, no-clean, halogen-free, Pb-free solder paste specifically formulated to achieve ultra-low voiding, especially in automotive applications.
For more information about Indium8.9HF and Indium10.1HF solder pastes and their use in automotive electronics, visit indiumstg.wpenginepowered.com/avoidthevoid or stop to see us at the show at booth #1K11.