Indium Corporation® is set to introduce its newest Heat-Spring® pattern—HSx. Designed for large area dies with warpage challenges and pressure limitations, HSx will be introduced at TestConX 2025, taking place March 3-5 in Mesa, Arizona.
As a global leader in high-performance metal thermal interface materials (TIMs), Indium Corporation will showcase the following selections from its array of high-performance metal TIM solutions:
Heat-Spring® HSx (New)
- Newest pattern designed for large area dies with warpage >200 microns
- Effective thermal conductivity of 16W/m-K at only 20psi with pure indium
- Designed for test heads where clamping forces are limited to <30psi
- Thickness ranging from 300 micron up to 1mm
- Available with or without a diffusion barrier to prevent staining of the die
Heat-Spring® HSD
- The original and best standard option for interfaces with flat, smooth, and parallel surfaces
- 專為緊密表面控制 >30psi 的介面所設計
Heat-Spring® High Profile Preforms
- 花紋設計可優化與非平面表面的接觸,提供 86W/mK
- Ideal for assemblies with an extruded, unfinished heat-sink
- Recommended for immersion cooling and burn-in applications
- 提供燒錄頭與 DUT 的均勻接觸
- 提供更均勻的熱傳導性
Heat-Spring® HSK
- 特別推薦用於需要多次插入的預燒應用
- 為高密度熱負載提供低電阻的均勻接觸
- 通常覆蓋一層薄薄的擴散屏障,作為燒機和測試應用的接觸面
- 無染色或裂紋
All Heat-Spring® products are recyclable and reclaimable.
To learn more about Indium Corporation’s metal TIMs for burn-in and test, visit our experts at booth #45 at TestConX, or online at https://www.indium.com/products/thermal-interface-materials/.
About Indium Corporation
Indium Corporation® is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, Germany, India, Malaysia, Singapore, South Korea, the United Kingdom, and the U.S.
For more information about Indium Corporation, visit www.indium.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.linkedin.com/company/indium-corporation/.