Indium Corporation will feature its ultra-reliable Indium8.9HF Solder Paste at SMT Hybrid Packaging, June 5-7, in Nuremberg, Germany.
Indium8.9HF Solder Paste is an air reflow, no-clean solder paste specifically formulated to accommodate the higher processing temperatures required by the SnAgCu, SnAg, and other alloy systems favored by the electronics industry.
The Indium8.9HF series delivers no-clean, halogen-free solder paste solutions designed to produce low-voiding—plus improved stability—during the printing process. Indium8.9HF:
- Demonstrates consistent printing and reflow performance for up to 12 months in refrigerated storage
- 실온에서 한 달 동안 보관해도 우수한 인쇄 및 리플로우 성능 유지
- 스텐실에 60시간 동안 방치한 후에도 뛰어난 응답성-일시 정지 인쇄 성능 제공
With all these qualities, Indium8.9HFsolder paste is able to enhance the reliability of the final product in three ways:
- Improved thermal conductivity and thermal reliability with industry-proven low-voiding performance
- Enhanced mechanical reliability when paired with Indium Corporation’s newest high-reliability alloy, Indalloy®276, which allows for a stable and consistent performance under a harsh environment (Indalloy®276 is ideal for operating temperatures equal to or greater than 150°C)
- Higher electrical reliability with an enhanced SIR
For more information about Indium8.9HF Solder Paste and its use in automotive electronics, visit indiumstg.wpenginepowered.com/avoidthevoid or stop to see us at the show at booth #4-301.
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.
인듐 코퍼레이션(Indium Corporation)에 대한 자세한 정보는indiumstg.wpenginepowered.com을방문하거나[email protected]으로 이메일을 보내 주시기 바랍니다. 또한www.facebook.com/indium또는@IndiumCorp에서 당사의 전문가 그룹인 From One Engineer ToAnother®(#FOETA)를 팔로우하실 수 있습니다.