Indium Corporation will feature its high-reliability precision AuSn Solder Preforms at the 48th NEPCON Japan, Jan. 16-18 in Tokyo, Japan.
Indium Corporation's AuSn preforms have the highest tensile strength of any solder, ensuring high-reliability for joining and sealing. The semiconductor-grade AuSn preforms are designed to meet industry challenges as devices continue to get smaller, with increasing power density and power ratings.
Depending on the alloy, gold-based solders have a melting point ranging from 280-1,064°C, making it compatible with subsequent reflow processes. Additionally, gold-based solders are resistant to corrosion, provide superior thermal fatigue resistance, and exhibit excellent joint strength.
Indium Corporation's Pb-free and RoHS-compliant AuSn solder preforms are available in a variety of standard and custom-engineered designs.
For more information about Indium Corporation's AuSn solder preforms, see our experts at the show or visit indiumstg.wpenginepowered.com/gold.
Indium Corporation은 전 세계 전자, 반도체, 박막 및 열 관리 시장에 최고의 소재를 제조 및 공급하는 기업입니다. 주요 제품으로는 솔더 및 플럭스, 브레이즈, 열 인터페이스 재료, 스퍼터링 타겟, 인듐, 갈륨, 게르마늄, 주석 금속 및 무기 화합물, NanoFoil® 등이 있습니다. 1934년에 설립된 이 회사는 중국, 말레이시아, 싱가포르, 한국, 영국, 미국에 글로벌 기술 지원 및 공장을 보유하고 있습니다.
인듐 코퍼레이션(Indium Corporation)에 대한 자세한 정보는indiumstg.wpenginepowered.com을방문하거나[email protected]으로 이메일을 보내 주시기 바랍니다. 또한www.facebook.com/indium또는@IndiumCorp에서 당사의 전문가 그룹인 From One Engineer ToAnother®(#FOETA)를 팔로우하실 수 있습니다.