Cleaning No-Clean Solder Paste Residues in SMT Assembly
Folks, There is a lot of interest in cleaning PCBs that have been assembled with no-clean solder pastes. Recently I discussed the topic with my ...
Folks, There is a lot of interest in cleaning PCBs that have been assembled with no-clean solder pastes. Recently I discussed the topic with my ...
Folks, I’m taking a few moments from Wassail Weekend , held annually in my village, Woodstock VT, “The prettiest small town in Americ...
Solder powder particle size and shape impacts the functionality of solder paste in many ways: printing/dispensing/dipping; solderballing; graping; voi...
Included in a solder paste‘s Product Data Sheet, among other things, are general guidelines which aid the customer in designing a...
Folks, I thought I would take a stab at listing the minuses, pluses, and “it’s a wash” aspects of assembling with lead-free (LF) sol...
Solder paste is made to be reflowed in the SMT process. Exactly HOW that is done is critical to your success. Included in the Product Data Shee...
Folks, Patty and Rob return from their honeymoon….... Patty had just finished some emails and was ready to head off to meet Rob and some of the...
Folks, After a bit of a break, the adventures of Patty, Rob, and The Professor continue: The plane droned on as it made its slow march from Detroit to...
Folks, Bob Landman’s comments to my tin whisker posts appear below. Friendly dialogue such as this helps us to all learn more and is ...
Graping is a phenomenon which appears as un-reflowed solder particles, typically seen on the surface of the solder joint. &nbs...
Patty was checking her email. She noticed a note from someone who had attended last night’s SMTA meeting. Patty had just been elected ...
Shhhh. Don’t tell anyone but I have a secret. The activators used in halogen-free solder pastes aren’t as effective as their h...