Elements of Indium by Indium Corporation: Wetting

In celebration of Indium Corporation’s 85th anniversary, the company will release monthly installments of the Elements of Indium Series—an educational program to raise awareness of the unique applications, abundance, and interesting properties of the 49th element.

Indium Corporation is the global leader for indium metal and associated technologies. Because of its unique properties with virtually limitless applications, indium metal is literally all around us.

Indium metal is a high-performing bonding material, especially when bonding non-metals such as quartz, glass, and glazed ceramics. Indium can also be cold welded to itself. It easily deforms under pressure and will fill voids between two surfaces, even at cryogenic temperatures.

For more information on indium metal, visit indiumstg.wpenginepowered.com/indium49.

Indium Corporation 是全球電子、半導體、薄膜和熱管理市場的主要材料製造商和供應商。產品包括焊錫和助熔劑、銅钎、熱介面材料、濺鍍靶材、铟、鎵、錫金屬和無機化合物以及 NanoFoil®。公司成立於 1934 年,擁有全球性的技術支援,工廠位於中國、印度、馬來西亞、新加坡、南韓、英國和美國。

For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another®(#FOETA), at www.facebook.com/indium or @IndiumCorp.