Indium Corporation experts will share their knowledge at the International Conference for Electronics Enabling Technologies (ICEET), June 4-6, Markham, Ontario.
Ed Briggs, Northeast Regional Sales Manager, will present Electrical Reliability for Automotive Assembly. He will discuss how the increasing amount of electronics in vehicles has escalated demands on automotive electrical systems in an industry with already challenging requirements. Briggs will also detail how Indium8.9HF Solder Paste provides improved electrical reliability and exceeds automotive requirements for SIR, electrochemical migration, and other harsh electrical requirements.
LED packaging has evolved from simple low-power packaging and gained many more applications in various industries. LEDs are now subject to challenges such as wide temperature ranges, high electrical currents, creep, and vibrations. Dr. Jie Geng, Research Metallurgist, will present High-Reliability Lead-Free Solder Alloys for High-Brightness LED Applications. In this presentation, he will examine the development of a novel high-reliability SnAgCuSb-based lead-free solder alloy designed to meet these challenges.
Power modules have continued to move toward higher power density, which requires die-attach materials to maintain long-term joint integrity in harsh high-temperature environments. Under temperatures >175°C, joint reliability can be jeopardized by defects driven by thermal or electromigration. Dr. HongWen Zhang, Manager, R&D Alloy Group, will present Microstructural Evolution of Solder Joints Under High-Temperature Service. His presentation examines the results of a die-attach materials test using four-lead free solders designed to examine the microstructural evolution of solder joints.
Briggs is an SMTA-certified process engineer. He earned his associate degree in chemical technology from Mohawk Valley Community College, where he received the Douglas J. Bauer Award for Excellence in Chemistry. In addition, he earned his Six Sigma Green Belt from Dartmouth College. Briggs joined Indium Corporation in 1990 and has held a variety of positions in production and technical support.
Dr. Geng has extensive experience on materials selection, design, processing, and characterization, especially on processing-structure-property relationships in various materials including ultra-high temperature alloys, lightweight alloys (Al and Mg), magnetic materials, and ceramics. He received his PhD in Metallurgy from the University of Surrey in the U.K. and has published more than 20 journal articles in the field of materials science and engineering. Dr. Geng also serves as a peer reviewer for numerous journals.
Dr. Zhang has extensive experiences in various aluminum (Al) alloys and fiber/particle-reinforced Al-based composite materials, and Al-rich and ZrHf-based amorphous alloys. He has published 20 or so journal publications in the field of metallurgy, materials science and engineering, physics, and mechanics. He was also invited as a peer reviewer for numerous journals. Dr. Zhang has a Six Sigma Green Belt from the Thayer School of Engineering at Dartmouth College. He is also a certified IPC Specialist for IPC-A-600 and IPC-A-610D.
To view papers authored by Indium Corporation experts, visit indiumstg.wpenginepowered.com/techlibrary.
Indium Corporation 是全球電子、半導體、薄膜和熱管理市場的主要材料製造商和供應商。產品包括焊料和助熔劑、銅钎、熱介面材料、濺鍍靶材、铟、鎵、錫金屬和無機化合物,以及 NanoFoil®。公司成立於 1934 年,擁有全球性的技術支援,工廠位於中國、馬來西亞、新加坡、南韓、英國和美國。
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.