Indium Corporation announces that it is now offering supplemental bar alloys for Indalloy291 wave solder pots designed to maintain recommended solder pot specifications.
The supplemental bar and bar chips are added to Indalloy291-containing solder pots that have fallen below or have elevated above the recommended specifications. This can be determined by solder analysis performed by Indium Corporation.
During wave soldering, when the molten solder contacts the air and manufacturing environment, a chunky layer of metal collects on the smooth surface of the molten soldersolder dross. Indium Corporation’s Dross Reduction Bar aids in the reduction of this solder dross build-up within Indalloy291 solder pots. By reducing dross formation, the Dross Reduction Bar also reduces the amount of solderable metal lost in the solder pot, providing the user a considerable cost-savings over time.
If instead during wave soldering the molten solder contacts a copper-containing PCB, such as an OSP board, the copper from the board can be pulled into the solder wave, increasing the solder pot’s copper content to an undesirable level. As copper levels gradually rise to become out-of-spec within an Indalloy291 solder pot, adverse effects to wetting performance and solder joint aesthetics can become more perceptible. Indium Corporation’s Replenisher Bar is used to bring the copper levels back within the recommended solder pot specifications.
Indium Corporation also offers a solder and solder dross recycle program to complete the usage cycle for bar solder. Up to 50% of bar solder used in wave soldering will be converted to dross, which still contains mostly usable metal. Indium Corporation can recycle these materials and return the metal value to you as a credit, or convert them to a usable bar for a fee. During an alloy switchover, use Indium Corporation’s recycling service to reclaim value on the pot dump and leftover bar. For more information about Indium Corporation’s solder and solder dross recycle program, please send an email to [email protected].
For more information, visit https://www.indium.com/products/solders/bar-solder/ or contact Robert McKerrow, Senior Product Specialist Flux-Cored Wire, Wave Solder Flux, and Bar Solder, here.
關於 Indium Corporation
Indium Corporation 是全球電子、半導體、薄膜和熱管理市場的主要材料精煉商、冶煉商、製造商和供應商。產品包括焊料和助熔劑、銅钎、熱介面材料、濺鍍靶材、铟、鎵、錫金屬和無機化合物,以及 NanoFoil 。公司成立於 1934 年,擁有全球性的技術支援,工廠分佈於中國、德國、印度、馬來西亞、新加坡、南韓、英國和美國。
如需進一步了解 Indium Corporation 的相關資訊,請造訪indiumstg.wpenginepowered.com或寄送電子郵件至Jingya Huang。您也可以在www.linkedin.com/company/indium-corporation/或@IndiumCorp 追蹤我們的專家專欄「From One Engineer To Another」(#FOETA)。