Indium Corporation earned Electronics Manufacturing (EM) World's Innovation Award for its new flux-cored wire for robotic and laser soldering. The award was presented on Thursday, March 18 in Shanghai, China, during Productronica China.
EM 創新獎計劃旨在表揚和慶祝電子行業的卓越成就,鼓勵企業達到最高標準,推動行業發展。
“We are honored to have CW-232 recognized by EM World,” said Robert McKerrow, senior product specialist. “CW-232 features a rare combination of fast-wetting and ultra-low spattering, attributes not often seen together in a highly active no-clean flux-cored wire. Its unique formulation delivers enhanced product efficiency, reducing the need for timely rework or cleaning that could impact yield.”
Indium Corporation 的CW-232是一種獨特配方的藥芯焊絲,透過提供額外的潤濕能力以達到更高的產量,從而滿足機器人和雷射焊接應用的嚴苛要求。
CW-232 在手焊應用中也非常有效。由於 CW-232 採用「無飛濺」技術,因此可避免助焊劑飛濺,以免灼傷操作員的雙手、損害機械人焊接機的視覺系統,或使成品不夠美觀。
Indium Corporation 的 CW-232 提供:
- 極低的飛濺性能
- 濕潤速度極快,甚至可焊接至嚴重塗污的表面
- 淺色殘留物
- 與無鉛和 SnPb 合金相容
- 與 HASL、浸銀、ENIG 及 OSP 表面處理相容
關於 Indium Corporation
Indium Corporation 是全球電子、半導體、薄膜和熱管理市場的主要材料精煉商、冶煉商、製造商和供應商。產品包括焊錫和助熔劑、銅钎、熱介面材料、濺鍍靶材、铟、鎵、錫金屬和無機化合物以及 NanoFoil®。公司成立於 1934 年,擁有全球性的技術支援,工廠位於中國、德國、印度、馬來西亞、新加坡、南韓、英國和美國。
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.
關於電子製造 (EM) 世界
EM World provides the latest information in the industry for professionals engaged in PCB component design, assembly, and testing in Asia; it has also become a contract manufacturer (EMS/ODM) and an OEM company and provides them with equipment, materials, and software. It is considered the authoritative magazine to learn about the latest development trend of SMT, electronic packaging, and interconnection technology with the overall solution supplier/agent.