Indium Corporation will feature an array of innovative thermal management solutions at SEMI-THERM, March 1317, in San Jose, CA.
Indium Corporation’s new line of innovative liquid metal pastes (LMP) has enabled a true liquid metal-based TIM solution capable of handling heat dissipation issues while maintaining long-term reliability. With higher viscosity than standard liquid metal, Indium Corporation’s next generation LMPs offer:
- Rth as low as 0.03K/W
- Predictable spreading characteristics
- Lower risk of pump-out
- Lower total costs
Indium Corporation’s Heat-Spring solutions, ideal for TIM2 applications, are a compressible interface between a heat source and a heat-sink. These indium-containing TIMs offer superior thermal conductivity over non-metalswith pure indium metal delivering 86W/mK. They are available as pure indium, pure indium clad with aluminum to prevent sticking to the device under test (DUT), indium-silver alloys, and indium-tin alloys.
Featured Heat-Spring products at SEMI-THERM:
- Are patterned to optimize contact with non-planar surfaces
- Provide uniform contact between the burn-in head and the DUT
- Provide more uniform thermal conductivity
- Clean with no residue
- Are recyclable and reclaimable
Indium Corporation’s GalliTHERM portfolio of gallium-based liquid metal solutions draws on the company’s more than 60 years of experience in manufacturing gallium-based liquid metals. These liquid metal TIMs are designed for both TIM1 and TIM2 applications. Liquid metal TIMs offer:
- 高導熱性可延長終端產品的壽命與可靠性
- 對大多數表面的介面阻抗低,可確保快速散熱
- Extraordinary wetting ability to both metallic and non-metallic surfaces
To learn more about Indium Corporation’s thermal management solutions, visit our experts at SEMI-THERM.
關於 Indium Corporation
Indium Corporation 是全球電子、半導體、薄膜和熱管理市場的主要材料精煉商、冶煉商、製造商和供應商。產品包括焊料和助熔劑;銅钎;熱介面材料;濺鍍靶材;铟、鎵、锗、錫金屬和無機化合物;以及 NanoFoil 。公司成立於 1934 年,擁有全球性的技術支援,工廠分佈於中國、德國、印度、馬來西亞、新加坡、南韓、英國和美國。
如需進一步了解 Indium Corporation 的相關資訊,請造訪indiumstg.wpenginepowered.com或寄送電子郵件至Jingya Huang。您也可以在www.linkedin.com/company/indium-corporation/或@IndiumCorp 追蹤我們的專家專欄「From One Engineer To Another」(#FOETA)。
About SEMI-THERM
SEMI-THERM is an international forum dedicated to the thermal management and characterization of electronic components and systems. It provides knowledge covering all thermal length scales from IC to facility level. The symposium fosters the exchange of knowledge between thermal engineers, professionals, and leading experts from industry as well as the exchange of information on the latest academic and industrial advances in electronics thermal management.