跳至內容

Indium Wire and Cryogenic Sealing

Indium wire is ideal for many sealing applications, especially cryogenic sealing. There are two main advantages to using indium wire in your cryogenic sealing applications:

  • It remains malleable at cryogenic temperatures
  • It is soft and pliable so it fills imperfections inmating metal surfacesand creates a hermetic seal

Most materials used for sealingthat workat standard operating temperatures will crack and break at the -150C cryogenic temperatures.

Often cryogenic, or anysealing, applications require that a seal be made inside a channel or other feature that isn't always flat and smooth.To illustrate how this works with indium,I used a piece of indium foil to show how it conforms to the surface of this penny.

Readmore about indium metal in generalor indium wire in particular.