Addressing a Defect of Poor wetting and Non-Spread of Solder Preforms
We’ve heard about the solder paste “graping” defect, but the same oxidation challenge occurs in other solder forms as well, such as ...
We’ve heard about the solder paste “graping” defect, but the same oxidation challenge occurs in other solder forms as well, such as ...
It seems like a fairly simple thing to do. What could be difficult about soldering a wire to a pad? Well, I hear three common complaints a...
The first time I was taught how to solder (as a child), I was told: “All the surfaces need to be mechanically cleaned and chemically cleaned.&rd...
While on a recent trip to Malaysia, I interviewed two colleagues regarding trends in semiconductor assembly. My previously-published interview with Sz...
Folks, There is a lot of interest in cleaning PCBs that have been assembled with no-clean solder pastes. Recently I discussed the topic with my ...
It is not often that we get a request for SIR (Surface Insulation Resistance) and/or ECM (Electro-Chemical Migration) results for a water washable/sol...
A few months back, while discussing tricks for hand soldering c-Si solar cells, I mentioned flux . One tip I didn’t mention is how to APPLY......
Indalloy Flux #2 is not the only option for soldering to Nitinol. There is also Indalloy Flux #3. Both fluxes are strong enough to clean the......
Maria Durham, Indium’s new Technical Specialist in Semiconductor and Advanced Assembly Materials, has been doing some research on indium lead (I...
a href="http://blogs.indium.com/blog/eric-bastow" target="blank”>img alt="Soldering to Nitinol with Flux 2" src=&quo...
We are often asked if it is possible to solder to stainless steel and, if so, what is the best procedure. As you may already know, stainless stee...
With regard to soldering or wetting (coating) with indium, we are often asked to comment on the oxide formation of indium and how to remove it.......