Pb-free Thermocouple Fix
A set of wires prepared for connection Properly joined thermocouple wires ......
A set of wires prepared for connection Properly joined thermocouple wires ......
Indium Corporation has just released a completely halogen-free wave solder flux that performs in a Pb-free process similar to its halogenated counterp...
A Chinese child sits amongst a pile of wires and e-waste. Children can often be found......
Typical profile for Pb-free sphere mounting for BGA assembly, adjusted using......
Folks, About two years ago it appeared that SAC305 (3.0% silver, 0.5% Cu, the balance tin) was becoming the de-facto standard for Pb-Free assembly. Wi...
The third day of the Device Packaging Conference has passed, with some interesting presentations from NXP, Amcor, and Atotech – to name a few. M...
Just incase you were wondering, here are the wetting results you can expect when soldering Pb-free spheres to different surface finishes. The chart sh...
Folks, I recently received this note: Hello Dr. Ron, A colleague of mine sent me the following article. I’m about to start the Pb-Free imple...
Folks, One of my closest and most respected colleagues in our industry is Jim Hall of ITM. Along with Phil Zarrow, also of ITM, Jim and......
Folks, I just chatted with iNEMI’s Jim McElroy about how iNEMI is working with companies concerned with high reliability and are partially RoHS...
Folks, If there is anything that I hope my blog does is to generate useful debate about the happenings in the electronics industry to help us all pros...