Indium Corporation, Nordson to Present Joint Paper at PCIM Asia

Indium Corporations Leo Hu, senior area technical manager East China, and Nordsons Jonas Chen, China Applications Manager of AXI Products, will co-present a joint paper on using solder-reinforced matrix preforms to increase reliability in power modules and the development of a novel X-ray algorithm to reduce false void detection at PCIM Asia, Sept. 9-11, Shenzhen, China.

In their presentation, Power Modules: Implementing Solder-Reinforced Matrix-Preforms for Increased Reliability & Unique Inline X-Ray Algorithms to Eliminate False Void Calls, Hu and Chen examine the benefits and cost-savings of using a solder-reinforced matrix-preform and how a unique X-Ray algorithm can enable 100% inspection of these traditionally challenging-to-inspect parts.

Cracking and solder layer delamination occurs faster in inhomogeneous solder joints due to stress concentration at thinner areas of the joint. Bondline control is, therefore, critical to prevent tilt and achieve a uniform solder joint. Unlike standard solder preforms and their higher cost of production due to necessary additional process steps, a solder preform engineered with an embedded reinforced matrix can achieve uniform solder bondline across the entire solder area, and eliminate all costs associated with the traditional wire spacer stitch and trim technique. Additionally, the innovative matrix design embedded in the solder significantly increases thermal cycling reliability by improving solder creep resistance and suppressing solder fatigue. 

Non-destructive inspection of voids in solder joints is crucial in the production process of power modules. While the matrix within the solder preformand the multiple overlapping solder layers already present within power modulescan present a challenge, autonomous X-ray inspection is the ideal method to solve this inspection task. A special approach was developed that involves an algorithm identifying typical features on the image for the reconstruction. To enable void inspection, the cooling pins (on the backside of the baseplate) are removed during the reconstruction, so that they do not appear on the slice images. Furthermore, due to the presence of the matrix in the solder preform, an additional step is necessary: a unique algorithm identifies and masks the matrix completely, so that it can be excluded from the analysis, enabling stable void inspection. 

Hu joined Indium Corporation in 2016 and is based in Suzhou, China. He has nearly 15 years of experience in semiconductor packaging and is a veteran in advanced assembly technology development, process improvement, and assembly materials applications. Hu has served in many roles at industry-leading outsourced assembly and test (OSAT) companies, including process engineer, project engineer, senior R&D engineer, and chief engineer. He has a masters degree in IC engineering from the Chinese Academy of Science and a bachelors degree in electronic information science and technology from Nankai University, Tianjin, China.

Chen joined the MATRIX team in 2012, before the Nordson acquisition. He is based in Shenzhen, China. He has nearly 10 years of experience with inline X-Ray inspection systems and is an expert in FATP (Final Assembly Testing), wire-bond, Power Hybrid inspection and in special applications. Chen has served MATRIX, and since 2015 Nordson, in many roles: he began as an engineer, he became a site leader afterwards and currently holds the position of Application Manager in China for the AXI products. 

インジウム・コーポレーションについて

インジウム・コーポレーションは、世界のエレクトロニクス、半導体、薄膜、熱管理市場向けの一流の材料精製、製錬、製造、サプライヤーである。製品には、はんだおよびフラックス、ろう材、熱界面材料、スパッタリングターゲット、インジウム、ガリウム、ゲルマニウム、スズの金属および無機化合物、NanoFoil などがある。1934年に設立され、グローバルな技術サポートと中国、ドイツ、インド、マレーシア、シンガポール、韓国、英国、米国に工場を持つ。

インジウム・コーポレーションに関する詳細については、indiumstg.wpenginepowered.comをご覧いただくか、Jingya Huang までメールでお問い合わせください。また、当社の専門家によるブログ「From One Engineer To Another (#FOETA)」を、www.linkedin.com/company/indium-corporation/または@IndiumCorp でフォローすることもできます。

About Nordson

The Test & Inspection division of Nordson is a global supplier of high-speed Autonomous X-ray Inspection systems (MATRIX AXI product line), available as inline machines and as inspection islands. The AXI systems are used to ensure the quality of critical electronic devices/components and electronic printed circuit boards. In addition, Nordson T&I supplies autonomous X-Ray inspection solutions for non-destructive testing of other non-electronic materials, such as batteries or medical parts, by using transmission (2D) and off-axis (2.5D) imaging and 3D computed tomography. The MATRIX AXI systems are a product line of Nordson Corporation (NASDAQ: NDSN), which also includes Manual X-Ray, Optical and Acoustic inspection systems of test and inspection products.

For more information about Nordson, visit www.nordson.com/en/divisions/matrix or [email protected].

About PCIM Asia

PCIM Asia, sister event of PCIM Europe in Nuremberg, Germany, offers unique opportunities in one of the fastest growing markets for power electronics. Established in 2002, PCIM Asia is the only specialized exhibition and conference platform in China for power electronics, intelligent motion, renewable energy, and energy management in the Asian market.