Products Compounds Indium Tin Oxide (ITO)

インジウム・スズ酸化物(ITO)

Indium tin oxide (ITO) is a composite material consisting of indium(III) oxide (In₂O₃) and tin (IV) oxide (SnO₂), typically in a 90:10 weight ratio. Known for its exceptional transparency and low sheet resistance, ITO is a preferred choice for flat panel displays and touch sensors. Indium Corporation offers premium, high-purity ITO products in bulk, suitable for fabricating sputter targets or creating ink formulations. Our ITO is provided in powder form, which can be compressed and sintered into sputter targets or used to produce ink-like coatings.

Powered by インジウム株式会社

  • Flexibility Over the Indium Oxide
  • Tight Control
  • Low Impurities, With a Powder Purity Level of >4N5
酸化インジウム・スズの前駆体である白い微粉末の山が、暗い背景を背景に透明なガラスシャーレの中に横たわっている。

While the 90/10 ratio of indium oxide to tin oxide is commonly preferred, we also offer alternative ratios to meet diverse needs. Our formulations range from 87% to 95% indium oxide by weight, enabling precise customization of sheet resistance and transparency in deposited films to suit specific customer requirements.

Our powder particles are precisely controlled to ensure a consistent size distribution, which plays a crucial role in the performance of our ITO products. The particle size and BET (surface area per unit mass) are closely related, and we carefully manage the BET value throughout our processes. We also provide this information with every shipment to support optimal performance in your applications.

Metallic impurities can greatly affect the electronic and optical performance of ITO films. We enforce stringent controls to minimize these impurities and provide detailed documentation of their levels in the Certificate of Analysis (COA) for each shipment.

白い円形の背景の上に、様式化された形と点が描かれた濃い緑色のアイコン。

Mobile phones

白い円形の背景の上に、様式化された形と点が描かれた濃い緑色のアイコン。

Balanced ratio

白い円形の背景の上に、様式化された形と点が描かれた濃い緑色のアイコン。

80%

白い円形の背景の上に、様式化された形と点が描かれた濃い緑色のアイコン。

4 eV

製品タイプd90d50d10BET m2/g (typical)
Type A – Standard32.0-44.013.2-24.02.7-8.02.4
Type D – Very Fine4.3-11.51.1-3.00.4-0.818.5

製品データシート

インジウム-スズ酸化物(ITO) PDS 97550 R12.pdf

関連アプリケーション

ITO is suitable for a wide range of applications.

化学合成を示す分子結合

化学合成

化学合成用のインジウムおよびガリウム化合物…

関連市場

Indium Corporation’s ITO is available for use in the following markets:

技術的なご質問や販売に関するお問い合わせはございませんか?当社の専門チームがお手伝いします。「From One Engineer to Another®」は当社のモットーであるだけでなく、卓越したサービスを提供するためのコミットメントでもあります。いつでもご連絡ください。つながりましょう!

この画像のalt属性は空です。ファイル名はscientist-with-microscope.pngです。

安全データシートをお探しですか?

技術仕様からアプリケーションガイダンスまで、必要なものすべてにアクセスできます。