Indium Corporation Introduces New ROL0 and Halogen-free Flux-cored Wire 

Indium Corporation today announced the global availability of CW-807RS, a new high-reliability, halide- and halogen-free flux-cored wire that improves wetting speeds and cycle times for electronics assembly and robot soldering applications. 

CW-807RSis a no-clean formula designed to maximize the solderability of a halogen-free cored wire solder flux. It is an upgraded version of Indium Corporation’s CW-807 formula, which has been popular with electronics assemblers and other customers for many years. This new halogen-free version will provide improved wetting speeds and contains the company’s industry-leading spatter control technology. 

Halogen-free CW-807RS delivers several benefits to users, including: 

  • Faster wetting speeds  
  • Clear residues for electronics assemblers that use high (>385°C) tip temperatures and tend to experience charring and tip build-up 
  • Improving cycle times in robotic soldering applications 

“The improved wetting and spatter performance make CW-807RS an excellent no-clean, high-reliability flux-cored wire option for many of our customers, especially in robotic soldering applications,” said Robert McKerrow, Product Manager for Flux-Cored Wire, Wave Solder Flux, and Bar Solder at Indium Corporation. “We’re excited to now offer this solution, combining cutting-edge innovation with proven technology to meet the needs of our customers.” 

CW-807RS provides exceptional benefits in manual and robotic soldering applications requiring an “L” IPC classification and halogen-free wire, as well as in manual and robotic soldering applications requiring extra wetting power to achieve higher throughput while remaining halogen-free. Additionally, the spatter control technology within the flux produces an aesthetically pleasing board post-soldering by leaving minimal spattering and a clear to light-colored residue. 

To learn more about Indium Corporation’s series of flux-cored wire products, visit https://www.indium.com/products/solder-wire/flux-cored-wire/

About Indium Corporation 

Indium Corporation is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, Germany, India, Malaysia, Singapore, South Korea, the United Kingdom, and the U.S. 