Indium Corporation experts Andreas Karch, Regional Technical Manager, Germany, Austria, and Switzerland, and Karthik Vijay, Technical Manager, Europe, Africa, and the Middle East, will share their industry knowledge during SMTconnect 2019 from May 7-9 in Nuremberg, Germany.
Vijay will present Automotive PCBA & No-Clean Solder Paste—Enhanced Electrical Reliability for High-Power Components. As automotive electrification and subsequent use of high-power components in under-the-hood electronics increases—as in 48V, HEV, and EV technologies—surface insulation resistance (SIR) specifications to assess the electrical reliability of the no-clean solder paste flux chemistry have become more stringent. Vijay willdiscuss the influence of no-clean flux chemistries on dendritic growth for high-power, low-standoff components as it pertains to these enhanced SIR conditions.
Karch will discuss Future-Proof Flux Systems in Solder Pastes: The Requirements for Electrical Reliability Are Increasing. Due to changes in the operating conditions of electronics assemblies, there are always new mission profiles for lifetime reliability. This also increases the demands on the materials used. In the area of "no-clean" solder pastes, the focus is on the SIR (surface insulation resistance) test as proof of the electrochemical duration reliability of these flux residues. For example, today's existing test duration has increased from 168 hours to 1,000 hours (+600%). Modern flux systems in solder pastes already have answers to these new challenges.
Vijay is based in the UK and manages Indium Corporation’s technology programs and technical support throughout Europe. His expertise is focused on solder paste, engineered solders, thermal interface materials, and semiconductor-grade electronics assembly materials. Vijay is active in several industry organizations, including IMAPS and the Surface Mount Technology Association (SMTA), and has presented at industry forums and conferences internationally. He earned his master’s degree in Systems Science and Industrial Engineering from Binghamton University, State University of New York.
As the Regional Technical Manager for Germany, Austria, and Switzerland, Karch provides support to Indium Corporation’s customers in those regions, including sharing process knowledge and making product recommendations. He has more than 20 years of automotive industry experience, including the advanced development of customized electronics. Karch is an ECQA-certified integrated design engineer, has a Six Sigma Yellow Belt, and was selected by the Austrian Patent Office as one of the 2014 recipients of the Top 10 Inventum Awards for an automotive LED assembly.
Indium Corporation will feature the solder products for high-reliability applications at the show, including Indium8.9HF solder paste, which exceeds all requirements for higher electronical reliability and has been approved for use in numerous automotive applications. To enable your process for 48V, please talk with our experts and find out more for your processes. For more information about Indium Corporation’s experts’ recent work, visit indiumstg.wpenginepowered.com/techlibrary or find them at the show in hall 5, booth 310.
Indium Corporation 是全球電子、半導體、薄膜和熱管理市場的主要材料製造商和供應商。產品包括焊料和助熔劑、銅钎、熱介面材料、濺鍍靶材、铟、鎵、錫金屬和無機化合物,以及 NanoFoil®。公司成立於 1934 年,擁有全球性的技術支援,工廠位於中國、馬來西亞、新加坡、南韓、英國和美國。
如需進一步了解 Indium Corporation,請造訪indiumstg.wpenginepowered.com或發送電子郵件至 [email protected]。您也可以在www.facebook.com/indium或@IndiumCorp 追蹤我們的專家團隊「From One Engineer ToAnother®」(#FOETA)。