Project 99 Wave Soldering Performance Proof: J-Standard Testing
The proof is in the data: Indium Corporation’s Project 99 wave fluxes have passed the latest test standards, J-STD-004B, are known to have the l...
The proof is in the data: Indium Corporation’s Project 99 wave fluxes have passed the latest test standards, J-STD-004B, are known to have the l...
They sound pretty but icicles can wreak havoc on electrical and solder reliability. Indium Corporation’s Project 99 wave soldering fluxes help d...
Residue is one of the most prevalent wave soldering defects......
Overcoming electro-migration issues can prevent dendrite growth and electrical leakage in the wave soldering process. Indium Corporation’s wave ...
Oxidation is more than just a cosmetic issue in wave soldering. Indium Corporation’s wave soldering fluxes defend against, and power through, ox...
Oxidation, residue, icicles and electro-migration are just a few of the persistent solder defects encountered during the wave soldering process. Meet ...
This video is for electronics assembly professionals who are looking to improve their wave soldering processes. It includes tools and resources that w...
This video is for electronics assemblers who currently are, or are considering, using a nitrogen reflow atmosphere during their process. It incl...
This video is for electronics assemblers who currently or are considering using nitrogen during their processes. It includes details regarding when ni...
The Soldering Station series is a continuation of a larger series entitled Wave Soldering (A Segmented Synopsis). Most recently we finished the Prehea...
With the exception of the automated system mentioned in my last post, there is little difference in the actual performance of the various forms of pre...
As discussed previously, the temperature of the preheater has little comparison with the actual temperature of the PCB. By implementing a dual p...