Indium Corporation will feature its MEMS microphone lid-attach Indium8.9HF Solder Paste at MEPTEC’s 15th Annual MEMS and Sensors Technology Symposium on June 6, in San Jose, Calif.
Indium8.9HF is a no-clean, halogen-free (no intentionally added, halogen-free flux) solder paste that enables dispensing of fine lines and shapes down to a width of less than 150 microns. Indium8.9HF provides reliable and consistent dispensing of a standard racetrack deposit using automated time/pressure or auger-based dispensing equipment.
Indium8.9HF eliminates failure modes, such as blow-hole, reduces solder creep, and increases solder joint shear strength. The flux is suitable for use with all standard Pb-free higher-melting alloys, such as those based on SnSb and SnAg.
For more information about Indium Corporation’s Indium8.9HF solder paste, visit indiumstg.wpenginepowered.com/indium8.9hf.
インジウム・コーポレーションに関する詳細については、indiumstg.wpenginepowered.comをご覧いただくか、[email protected] までメールでお問い合わせください。また、当社の専門家による「From One Engineer ToAnother®(#FOETA)」を、www.facebook.com/indiumまたは@IndiumCorp でフォローすることもできます。