Indium Corporation has released NC-702, a no-clean, near-zero residue, halogen-free adhesive solution designed for holding parts in place during placement and reflow processes.

Designed for use in a formic acid reflow environment, NC-702 is specially formulated with high tack to hold a die, chip, or solder preform in place without movement, creating a low-cost tooling-free solution over pick and place investments. While NC-702 has the tack strength to hold materials in place, the material is completely evaporated out during reflow, eliminating the time-consuming post-reflow residue cleaning steps. Benefits include:

  • No evidence of contamination during reflow, enabling use in formic acid reflow environments without risk of damaging equipment
  • Flexible application method via dipping, dispensing, or jetting, potentially reducing process costs
  • Minimal voiding present and good soldering performance; although classified as an adhesive solution, NC-702 does not negatively affect soldering performance
  • Compatible with molding and underfill material
  • Compatible with most common SAC alloys

For more information about NC-702, contact Indium Corporation Product Specialist Evan Griffith

关于铟泰铟泰公司

Indium Corporation is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil. Founded in 1934, the company has global technical support and factories located in China, Germany, India, Malaysia, Singapore, South Korea, the United Kingdom, and the U.S.

如需了解铟泰公司更多信息,请访问indiumstg.wpenginepowered.com或发送电子邮件至Jingya Huang。您还可以关注我们的专家团队“From One Engineer To Another”(#FOETA),访问www.linkedin.com/company/indium-corporation/或关注@IndiumCorp