Indium Corporation has released a new halogen-free, no-clean ROL0 flux specifically developed for PCB assembly hand soldering and rework applications. 

TACFlux® 020B-RC passes SIR testing in the unreflowed state. Oftentimes during hand soldering and rework, the flux may not be heated properly due to spot heating methods, thus the flux is not adequately activated. TACFlux® 020B-RC is designed to solve this problem and avoid reliability concerns such as dendritic growth over time. 

TACFlux® 020B-RC joins Indium Corporation's versatile offering of specialty fluxes designed to provide solutions for current and evolving industry challenges. Benefits of TACFlux® 020B-RC include: 

  • Passes J-STD-004B SIR testing in the unreflowed state
  • Halogen-free per IEC 61249-2-21 test method EN14582
  • Outstanding wetting performance on difficult to solder metallizations 
  • Designed for no-clean applications, but flux can be removed using a commercially-available flux-cleaner

For more information about TACFlux® 020B-RC, visit indiumstg.wpenginepowered.com/flux-and-epoxy/tacky-flux.

Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.

如需了解铟泰公司更多信息,请访问indiumstg.wpenginepowered.com或发送电子邮件[email protected]。您还可以通过www.facebook.com/indium@IndiumCorp 关注我们的专家团队“From One Engineer ToAnother®”(#FOETA)。