Indium Corporation will feature products from its line of proven gallium-based liquid metal thermal solutions at SEMI-THERM, March 21-25, San Jose, Calif., U.S.
Indium Corporation is a leader in high-performance liquid metal-based thermal interface materials (TIM) with advanced knowledge and experience in high-volume TIM0, TIM1, and TIM2 applications.
Indium Corporation’s Gallitherm portfolio of gallium-based liquid metal solutions draws on the company’s more than 60 years of experience in manufacturing gallium-based liquid metals. Indium Corporation also offers significant global technical support to help customers ensure their liquid metal thermal solutions meets their application needs with low- and high-volume production available in the U.S. and Asia.
Indium Corporation offers a number of innovative high-performance metal TIM solutions. With its portfolio of alloys that are liquid at or near room temperature, Indium Corporation’s liquid metal TIMs are designed to offer superior thermal conductivity for both TIM1 and TIM2 applications. Liquid metal TIMs offer:
- 高热导率,可延长最终产品的使用寿命并提高其可靠性
- 与大多数表面之间具有较低的界面电阻,可确保其快速散热
- 对金属和非金属表面均具有卓越的润湿
液态金属 有多种合金可供选择,包括 InGa 和 InGaSn。
Indium Corporation’s m2TIMTM combines liquid metal with a solid metal preform to provide reliable thermal conductivity for heat dissipation without the need for a solderable surface. The presence of a solid solder preform absorbs and contains the liquid alloys while improving thermal conductivity.
Available in InGa and InGaSn, this m2TIMTM hybrid approach provides extraordinary wetting ability to both metallic and non-metallic surfaces and low interfacial resistance. It also eliminates the risk of pump-out of the liquid alloy.
For more information, visit Indium Corporation’s experts at the show at booth #500.
关于铟泰铟泰公司
Indium Corporation is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil. Founded in 1934, the company has global technical support and factories located in China, Germany, India, Malaysia, Singapore, South Korea, the United Kingdom, and the U.S.
如需了解铟泰公司更多信息,请访问indiumstg.wpenginepowered.com或发送电子邮件至Jingya Huang。您还可以关注我们的专家团队“From One Engineer To Another”(#FOETA),访问www.linkedin.com/company/indium-corporation/或关注@IndiumCorp。
About SEMI-THERM
SEMI-THERM is an international forum dedicated to the thermal management and characterization of electronic components and systems. It provides knowledge covering all thermal length scales from IC to facility level. The symposium fosters the exchange of knowledge between thermal engineers, professionals, and leading experts from industry as well as the exchange of information on the latest academic and industrial advances in electronics thermal management.