Indium Corporation’s EZ-Pour Gallium Trichloride Simplifies Room Temperature Processes

Indium Corporation's EZ-Pour® Gallium Trichloride (GaCl3) simplifies the use of gallium trichloride by allowing the user to easily transfer the product from one container to another at room temperature.

Traditional gallium trichloride is solid at room temperature and often forms clumps or sticks together during storage and use. This inhibits the efficient and consistent materials transfer between vessels and processing equipment. EZ-Pour® Gallium Trichloride’s unique free form solves this challenge by eliminating clumping and enabling fast, efficient, safe, and accurate transfer.

For more information about EZ-Pour® Gallium Trichloride, visit indiumstg.wpenginepowered.com/gallium-trichloride.

铟泰公司 面向全球电子、半导体、薄膜、热管理及太阳能市场的顶级材料制造商和供应商。 产品包括焊料和助焊剂;硬钎焊;热界面材料;溅射靶材;铟、镓(Ga)、锗和锡的金属及化合物;以及NanoFoil®。铟泰公司成立于1934年,拥有全球技术支持网络,并在中国、马来西亚、新加坡、韩国、英国和美国设有工厂。

如需了解铟泰公司更多信息,请访问indiumstg.wpenginepowered.com或发送电子邮件[email protected]。您还可以通过www.facebook.com/indium@IndiumCorp 关注我们的专家团队“From One Engineer ToAnother®”(#FOETA)。