Indium Corporation Expert Receives SMTA Technical Distinction Award

Indium Corporation R&D Manager of the Alloy Group and Principal Research Metallurgist Dr. HongWen Zhang was presented with SMTA’s prestigious Technical Distinction Award during an awards ceremony on October 9 at SMTA International in Minneapolis, MN. The Technical Distinction Award recognizes individuals who have made significant and continuing technical contributions to SMTA over a period of at least three years.

“I am deeply honored to receive the Technical Distinction Award as it not only acknowledges my dedication to advancing SMT technology, but also the collaborative spirit of our industry,” said Dr. Zhang. “Together we’ve pushed the boundaries of what’s possible, and I’m excited to continue this journey of innovation and discovery.” 

As manager of the alloy group in Indium Corporation’s R&D department, Dr. Zhang’s focus is on the development of the varieties of Pb-free solder materials and the associated technologies for low-temperature, high-temperature and/or high-reliability applications. He was instrumental in inventing the Durafuse technology to combine the merits of constituents to improve wetting, reduce processing temperatures, modify the bonding surface, and control the joint’s morphology, thus improving reliability. As principal metallurgist, he is also responsible for expanding metallurgical innovation. He and his team are responsible for using metallurgical insight to develop new products, implement improvements to existing processes and products, and measure results.

Dr. Zhang has a bachelor’s degree in metallurgical physical chemistry from Central South University of China, a master’s degree in materials and engineering from the Institute of Metal Research, Chinese Academy of Science, and a master’s degree in mechanical engineering and a Ph.D. in material science and engineering from the Michigan Technological University. He has a Six Sigma Green Belt from the Thayer School of Engineering at Dartmouth College, and is a certified IPC Specialist for IPC-A-600 and IPC-A-610, as well as a certified SMT Process Engineer. He has extensive experience in various aluminum (Al) alloys and fiber/particle reinforced Al-based composite materials, and Al-rich and ZrHf-based amorphous alloys. He has co-authored two book chapters on high-temperature lead-free bonding materials, has had a dozen patents granted, and has been published in more than 20 journals in the fields of metallurgy, materials science and engineering, physics, electronics materials, and mechanics.

关于铟泰铟泰公司

铟泰公司 是面向全球电子、半导体、薄膜及热管理 顶级材料精炼商、冶炼商、制造商和供应商。产品包括焊料和助焊剂;硬钎焊;热界面材料;溅射靶材;铟、镓(Ga)、锗和锡等金属及化合物;以及NanoFoil 。公司成立于1934年,拥有全球技术支持网络,并在中国、德国、印度、马来西亚、新加坡、韩国、英国和美国设有工厂。