Indium Corporation's germanium reclaim and recycle program enables customers to increase their return on materials by providing credit for diverting spent germanium from the waste stream.

Germanium, used in the production of fiber optic cables, optical lenses and wafers, and catalysts in polyethylene (plastic) production, is typically not completely consumed during the process. The remaining germanium can be reclaimed and recycled, enhancing process efficiency and providing a financial return.

Indium Corporation also offers reclaim and recycle programs for indium and indium alloys, solder pot dross and contaminated solder, and indium tin oxide (ITO) and indium gallium zinc oxide (IGZO) from sputtering targets.

For information about Indium Corporation’s reclaim and recycling programs, visit indiumstg.wpenginepowered.com/reclaim-and-recycle.

铟泰公司 面向全球电子、半导体、薄膜、热管理及太阳能市场的顶级材料制造商和供应商。 产品包括焊料和助焊剂;硬钎焊;热界面材料;溅射靶材;铟、镓(Ga)、锗和锡的金属及化合物;以及NanoFoil®。铟泰公司成立于1934年,拥有全球技术支持网络,并在中国、马来西亚、新加坡、韩国、英国和美国设有工厂。

如需了解铟泰公司更多信息,请访问indiumstg.wpenginepowered.com或发送电子邮件至 [email protected]。您还可以通过www.facebook.com/indium或@IndiumCorp 关注我们的专家团队“From One Engineer ToAnother®”(#FOETA)。