Indium Corporation has launched InFORMS® ESM02, a reinforced matrixed solder composite specifically designed to produce consistent bondline thickness for die-level attach applications.
Indium Corporation's InFORMS® ESM02 is a reinforced solder fabrication that produces a high-reliability solder joint with increased thermal and mechanical performance.
Until recently, InFORMS® technology was only applied at the baseplate level. New production capabilities have expanded its use to the die-level with a bondline of 50μm. Other benefits of InFORMS® include:
- Drop-in replacement for other bondline control methods
- Increased lateral strength
- Bondline co-planarity
- Improved thermal cycling reliability
- Available in ribbon and preforms
|
Standard InFORMS® Configurations |
|
|
Description |
Standoff (Microns) |
|
LM04 |
100 |
|
LM06 |
150 |
|
LM08 |
200 |
|
SM04 |
100 |
|
ESM03 |
75 |
|
ESM02 |
50 |
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.