Indium Corporation introduces Indium12.8HF as it continues to develop innovative solder paste solutions to meet customers’ current and emerging needs. Indium12.8HF is a versatile paste engineered to deliver exceptional jetting and microdispensing performance on a variety of systems.
Indium12.8HF is a no-clean, halogen-free solder paste that is inherently compatible with Indium Corporation’s best-selling solder pasteIndium8.9HFand is optimized for long-term jetting and microdispense applications. Originally formulated for micro-LED applications, Indium12.8HF has proven to be useful in a wide range of applications requiring precision dot diameter/line width deposits down to 80m.
此外,铟12.8HF:
- 符合 IPC J-STD-004B 第 1 修正案 ROL0 的要求
- Offers exceptional electrical reliability
- Minimizes graping and similar reflow issues with a unique flux oxidation barrier formulation
- Delivers aesthetically pleasing clear residue with minimal flow-out
- 与同类焊膏相比,回流焊飞溅最小
- Long working (syringe) life
To learn more about Indium Corporation’s new jetting and microdispensing paste, visit indiumstg.wpenginepowered.com/jetting-paste.
关于铟泰铟泰公司
Indium Corporation is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil. Founded in 1934, the company has global technical support and factories located in China, Germany, India, Malaysia, Singapore, South Korea, the United Kingdom, and the U.S.
如需了解铟泰公司更多信息,请访问indiumstg.wpenginepowered.com或发送电子邮件至Jingya Huang。您还可以关注我们的专家团队“From One Engineer To Another”(#FOETA),访问www.linkedin.com/company/indium-corporation/或关注@IndiumCorp。