跳至内容

Indium Corporation Features InFORMS Reinforced Solder Preforms at PCIM Europe 2017

Indium Corporation will feature its reinforced solder alloy fabrications, InFORMS®, at PCIM Europe 2017, May 16-18, in Nuremberg, Germany.

Indium Corporation is redefining solder with its InFORMS solder preforms. InFORMS are a composite preform consisting of solder and a reinforcing matrix that, together, increase lateral strength and bondline co-planarity while improving thermal cycling reliability.

When InFORMS were used to solder a DBC to the baseplate of an IGBT, one study showed:

  • 4x improved thermal cycling reliability compared to a solder preform-only approach
  • 2x improved thermal cycling reliability compared to a solder preform + Al wirebond stitch approach
  • Reduced voiding (<1%)
  • 拥有成本更低 - InFORMS 可直接替代标准预型件或焊膏,无需额外的工艺步骤或设备

For more information about InFORMS, visit indiumstg.wpenginepowered.com/informs or see Indium Corporation at booth 7-315.

如需了解铟泰公司更多信息,请访问indiumstg.wpenginepowered.com或发送电子邮件[email protected]。您还可以通过www.facebook.com/indium@IndiumCorp 关注我们的专家团队“From One Engineer ToAnother®”(#FOETA)。