Skip to content

Indium Corporation Releases New Research Kit for Soldering to Gold

Indium Corporation has released a new solder research kit designed for soldering to gold plating using indium-based alloys.

Gold is often used in electronics assembly because it resists oxidation and solders readily. This makes gold ideal for plating contact surfaces for switches and connectors.

The more commonly used tin-based solder alloys rapidly scavenge or dissolve the gold during the reflow process, leading to the destruction of gold conduction patterns. Tin-based alloys also result in crack-inducing platelets within the solidified solder joint. Indium-based alloys, especially those in the indium-lead (InPb) family, cause appreciably less gold scavenging damage than tin-lead (SnPb) solders.

The Soldering to Gold Research Kit allows you to choose three different alloys from seven that are offered for the kit. The alloys come in the form of 0.76mm (0.030”) solid-core wire and represent melting temperatures ranging from 143-310°C. The kit also offers two compatible fluxes – TACFlux® 007 and TACFlux® 012.

Order your research kit at www.buy.solder.com. If you want more information on how to solder to gold, visit indiumstg.wpenginepowered.com/soldering-to-gold. For assistance on selecting the best alloys for your application, visit Indium Corporation’s Solder Alloy Selector Guide at indiumstg.wpenginepowered.com/solder-alloy-guide or contact our technical support team at [email protected].

Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, Indium has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.

For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.