Indium Corporations Durafuse LT Earns Mexico Technology Award

Indium Corporation earned the Mexico Technology Award for its patent-pending Durafuse™ LT low-temperature alloy system.

The Mexico Technology Awards, sponsored by Mexico EMS, recognizes the best electronics manufacturing innovations in the electronics manufacturing industry in Mexico produced by OEM manufacturing equipment and materials suppliers over the last year.

The awards are designed to promote best practices in technical innovation, manufacturing quality, and productivity by celebrating the companies and people achieving high standards and driving the industry forward.

“Indium Corporation continues to be honored by the recognition Durafuse™ LT has received from the electronics assembly industry,” said Tim Twining, Vice President of Marketing. “We developed Durafuse™ LT as an innovative solution to the challenges of conventional low-temperature solders as part of our belief that materials science changes the world. Because of it, we now have a proven product that can address the electronics assembly challenges of today and the future.”

Durafuse™ LT is a novel, low-temperature alloy system designed to provide high-reliability in low-temperature applications that need to reflow below 210°C. Where traditional low-temperature solders can produce brittle solder joints that are susceptible to drop shock failures, Durafuse™ LT provides improved drop shock resilience, outclassing BiSn or BiSnAg alloys, and performing better than SAC305 with optimum process setup. Durafuse™ LT:

  • 为热敏元器件 柔性聚合物提供解决方案
  • 防止处理器元器件 多层电路板因热膨胀而变形
  • 符合低温 对阶梯焊接 的要求,特别是在射频屏蔽件的安装方面,以及返修 应用

Learn more about Indium Corporation’s innovative low-temperature technology at indiumstg.wpenginepowered.com/durafuse.

Indium Corporation is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, India, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.

For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.