PCB Assembly Solder Pastes
锡铅焊膏
Indium Corporation’s tin-lead solder pastes have long been trusted by top emergency medical service providers for their exceptional solderability and reliable performance, a legacy that began with our renowned NC-SMQ92J. These pastes are specifically formulated to meet the strict requirements of electronics manufacturing, providing strong and durable joints in applications ranging from industrial equipment to complex military and aerospace assemblies.
技术支持:铟泰公司
- 成熟可靠
- 卓越性能
- 卓越的技术支持

产品概览
大量选择
Indium Corporation offers a number of SnPb solder pastes for circuit board assembly and high-Pb applications common in semiconductor packaging.
证明
凭借数十年成熟的助焊剂技术,我们的焊膏可为客户提供最高的终端产量。
广泛兼容
我们的大多数助焊剂与含铅合金和其他产品(如带芯线)兼容。
多用途
From no-clean and water-wash to RMA, our tin-lead solder pastes are designed to work for a variety of applications.
锡铅膏产品
我们有大量可与含铅合金完美配合的助焊剂,以及包括包芯线在内的其他产品。
No-Clean
| 产品名称 | 价值主张 |
|---|---|
| 铟8.9HF | Best all-around halogen-free paste |
| NC-SMQ92H | 最大限度提高打印性能的 NC-SMQ92J 改良版 |
| NC-SMQ92J | Industry-leading solder paste with a soft residue that reduces false failures at ICT |
| NC-SMQ51SC | Exceptional stencil life and tack strength, and consistent print definition in ultra-fine pitch applications |
| NC-SMQ80 | Specialty solder paste (InPb) for soldering to gold surfaces |
Water-Soluble
| 产品名称 | 价值主张 |
|---|---|
| 铟6.6HF | Superior wetting to a variety of surface finishes and exhibits the best voiding performance |
| 铟6.5R | A versatile, low-voiding solder paste (InPb) |
| 铟6.3 | A low voiding solder paste with a wide reflow window |
RMA
| 产品名称 | 价值主张 |
|---|---|
| RMA-155 | Low voiding solder paste with a wide reflow window |
| RMA-SMQ51AC | A no-clean RMA solder paste with excellent soldering performance |
产品数据表
铟 8.9HF(锡锑)焊膏 PDS 99684 R0.pdf
相关应用
相关市场
Indium Corporation’s tin-lead solder pastes are widely used across industries such as telecommunications, automotive electronics, some consumer electronics, and aerospace.
专家支持,结果可靠
您有技术问题或销售咨询吗?我们的专业团队随时为您提供帮助。From One Engineer to Another®不仅是我们的一句口号,更是我们致力于提供卓越服务的承诺。只要您需要,我们随时待命。让我们联系吧!

寻找安全数据表?
您所需的一切——从技术规格到应用 ——都可在此一站式获取。

您的成功
是我们的目标
借助最新的材料、技术以及专家应用 优化您的生产流程。一切都始于与我们团队的联系。