焊料
焊料块
Indium Corporation manufactures high-quality, very-low-oxide content, extruded bar solder for wave, fountain, and dip soldering applications. We use only “conflict-free” grade-A tin, per ASTM B32.
技术支持:铟泰公司
- 无冲突
- 低氧化物
- 符合或超过 J-STD-006 标准


概述
功能和优点
Indium Corporation bar solder alloy composition and purity meets, or exceeds, the requirements of ASTM B32, IPC J-STD-006, and JIS Z 3282, as well as all other similar industry and customer specifications.
Bar solder chips are also available and are commonly used to fill smaller solder pots or to quicken the melting of solder in a new solder pot. The greater surface area of the chips allows for better heat transfer between the solder pot and the metal.
Bar Solder Products
Alloys for dip tinning and other applications: 50Sn50Pb, 40Sn60Pb, 30Sn70Pb, 10Sn90Pb, 5Sn95Pb, 96.5Sn3.5Ag, 95Sn5Sb, SAC105, and others upon request.
产品数据表
补给条 PDS 99843 R1.pdf
Indalloy®291焊条 PDS 99834 R2.pdf
渣滓还原棒 PDS 99826 R0.pdf
Bar Solder Chips PDS 99050 R1.pdf
相关应用
Bar Solder can be used in various applications.
相关市场
Indium Corporation’s Bar Solder products are a great option for many markets.
专家支持,结果可靠
您有技术问题或销售咨询吗?我们的专业团队随时为您提供帮助。From One Engineer to Another®不仅是我们的一句口号,更是我们致力于提供卓越服务的承诺。只要您需要,我们随时待命。让我们联系吧!

寻找安全数据表?
您所需的一切——从技术规格到应用 ——都可在此一站式获取。

您的成功
是我们的目标
借助最新的材料、技术以及专家应用 优化您的生产流程。一切都始于与我们团队的联系。