Indium Corporation’s Karthik Vijay, Technical Manager for Europe, Africa, and the Middle East, will present at the InnovationsFORUM Hungary on May 25 in Budapest, Hungary.
Karthik will present Minimizing QFN Voiding During SMT Assembly. This presentation provides insight into how reflow profile, stencil thickness, and flux chemistry type impact voiding levels.
Innovations Forum is an event for electronics manufacturers to learn the most advanced technologies, materials, and processes. You can register for free by visiting epp-europe.industrie.de/events-tutorials/innovationsforum-hungary/#registration and using the code IFHIndium2017.
Karthik is based in the UK and manages Indium Corporation’s technology programs and technical support throughout Europe. His expertise is focused on solder paste, engineered solders, thermal interface materials, and semiconductor-grade electronics assembly materials. Karthik is active in several industry organizations, including IMAPS and the Surface Mount Technology Association (SMTA), and has presented at industry forums and conferences internationally. He earned his master’s degree in systems science and industrial engineering from Binghamton University, State University of New York.
インジウム・コーポレーションは、世界のエレクトロニクス、半導体、薄膜、および熱管理市場に材料を供給する一流メーカーです。製品には、はんだおよびフラックス、ろう材、熱界面材料、スパッタリングターゲット、インジウム、ガリウム、ゲルマニウム、スズの金属および無機化合物、NanoFoil®などがあります。1934年に設立されたインジウムは、グローバルな技術サポートと中国、マレーシア、シンガポール、韓国、英国、米国に工場を有しています。
インジウム・コーポレーションに関する詳細については、indiumstg.wpenginepowered.comをご覧いただくか、[email protected] までメールでお問い合わせください。また、当社の専門家による「From One Engineer ToAnother®(#FOETA)」を、www.facebook.com/indiumまたは@IndiumCorp でフォローすることもできます。