Several Indium Corporation technology experts will present at the Surface Mount Technology Association’s International Conference and Exhibition (SMTAi) on October 15-17 in Fort Worth, Texas.
Dr. Ning-Cheng Lee, Vice President of Technology, will give three presentations.
Voiding and Reliability of BGA Assemblies with SAC and 57Bi42Sn1Ag Alloys explores replacing SAC solders with BiSnAg as a low-cost solution. The joint mechanical strength, drop test performance, and voiding performance of these alloys were evaluated against their reflow profile.
Corrosion Resistance of High Melting Lead-free BiAgX Solder Joints compares the corrosion resistance of Pb5/Sn2.5/Ag and SAC305 with BiAgX®, a drop-in lead-free solder paste solution for high temperature die-attach applications.
The Second Generation Shock Resistance and Thermally Reliable Low Ag SAC Solder Doped with Mn discusses the considerable improvement in shock resistance and thermal fatigue performance of a new soldering alloy doped with Mn.
Tim Jensen, Product Manager of PCB Assembly Materials, will present Alloy and Process Optimization for Low-Ag Solders. This presentation reviews the differences and impact of alternative alloys to SAC305 on electronics assembly.
Jensen will also give a workshop titled Soldering Technology for SMT: Achieving High Yields and Reliability. This workshop provides a detailed discussion of solder materials, components, and PCBs, and how each is important when producing a complete electronics product that meets current and future legislative restrictions. He will also include a detailed discussion of process optimization and defect elimination in the assembly process.
Dr. Ron Lasky, Senior Technologist, will present Using Weibull Analysis to Interpret Failure Data in Electronics Assembly Stress Testing. This presentation explores how to use the Weibull function to analyze failure data in electronics assembly. Lasky will discuss several case studies that include multiple failure modes and early first fails.
Brook Sandy-Smith, Product Support Specialist – PCB Assembly Materials, will present four papers:
Optimizing Assembly of QFNs explores several tested and proven strategies to minimize voiding in QFN assemblies, including thermal pad design and patterning, via placement, and addition of a flux-coated solder preform.
Measuring Tiny Solder Deposits with Accuracy and Repeatability discusses advancements in paste deposit inspection equipment, allowing for more accurate characterization of tiny solder deposits. This is especially important to ensure repeatability of miniaturized assemblies.
Probe Technologies to Improve First Pass Yield looks at the impact that flux residue permeability has on the first-pass yield results. It also discusses the role that aperture design has on creating an optimal surface for contact.
Productivity and Profitability Assessment of Improved Pin Probe Testing uses a case study to compare solder pastes with different flux residue characteristics and first-pass yields for in-circuit tests. Sandy-Smith also discusses factors that impact profitability, such as probe cleanliness, the number of actuations required to ensure repeatable testing, and false positives.
Additionally, Indium Corporation technical experts will be chairing several sessions.
リー博士は世界的に著名なはんだ付けの専門家であり、SMTAの特別会員でもある。高温ポリマー、マイクロエレクトロニクス用封止材、アンダーフィル、接着剤の開発に豊富な経験を持つ。現在の研究テーマは、エレクトロニクスおよびオプトエレクトロニクス用途の相互接続およびパッケージング用先端材料で、高性能と低所有コストの両方に重点を置いている。
ジェンセンはSMTA認定のプロセスエンジニアである。クラークソン大学で化学工学の学士号を取得。15年以上にわたり顧客と協力してSMTプロセスラインのトラブルシューティングと最適化を行い、ヘッドインピロー、グレーピング、QFNボイドなどの問題を解決してきた。何百ものSMTラインに直接携わることで、各顧客固有の要件を理解し、技術論文の執筆や技術出版物への寄稿を通じて、専門知識を容易に共有している。また、複数のIPC規格開発委員会にも積極的に参加している。
Dr. Lasky, holder of the prestigious SMTA Founder’s Award, is a world-renown process expert and an Instructional Professor at Dartmouth College. He has over 25 years of experience in electronics and optoelectronic packaging and assembly. He has authored or edited five books and numerous technical papers and holds several patent disclosures. Dr. Lasky also authors a technology blog, which can be found at indiumstg.wpenginepowered.com/drlasky.
Sandy-Smith serves as a technical liaison between Indium Corporation’s customers and internal departments, such as research and development and production, to ensure the best quality and selection of products. She earned two degrees from the international engineering program at the University of Rhode Island: one in chemical engineering with a focus on materials, the other in German language.
インジウム・コーポレーションは、世界のエレクトロニクス、半導体、太陽電池、薄膜、熱管理市場に材料を供給する一流メーカーです。製品には、はんだ、プリフォーム、フラックス、ろう材、スパッタリングターゲット、インジウム、ガリウム、ゲルマニウムの金属および無機化合物、NanoFoil®などがある。1934年に設立されたインジウムは、グローバルな技術サポートと中国、シンガポール、韓国、英国、米国に工場を有しています。
インジウム・コーポレーションに関する詳細については、indiumstg.wpenginepowered.comをご覧いただくか、[email protected] までメールでお問い合わせください。